Precipitation-hardened aluminium alloys typically obtain their strength by forming second-phase particles, which, however, often have a negative effect on formability. To enable both lightweight construction and forming of complex parts such as body panels, high strength and formability are required simultaneously. Cluster hardening is a promising approach to achieve this. Here, we show that short thermal spikes, denoted as up-quenching, increase aging kinetics, which we attribute to the repeated process of vacancies being formed at high temperatures and retained when cooled to lower temperatures. Combined with further heat treatment, the up-quenching process promotes rapid and extensive cluster formation in Al-Mg-Si alloys, which in turn generates significant strengthening at industrially relevant heat treatment time scales. The high elongation values also observed are attributed to reduced solute depleted zones along grain boundaries.
Sn-alloying, by deploying comparatively high vacancy binding energy, mitigates the undesired natural aging behavior of 6xxx-alloys. Targeted selection of pre-aging parameters can have a positive influence on natural aging and paint-bake performance. In this study, we aimed to combine the two approaches of Sn-alloying and pre-aging. Our results indicate that alloys modified with 100 at.-ppm Sn require altered heat treatment. In terms of solution aging and quenching, we show that the cooling rate needed depends on the types of alloy. The rate must be adapted, according to the number of intermetallic particles, to guarantee a sufficiently high level of Sn atoms in solid solution. The rather high number of intermetallic phases in alloy EN-AW-6061 means that it requires fast quenching, while the comparatively low number of precipitate-forming elements in alloy EN-AW-6016 makes it less sensitive to quenching variations. We also show that Sn reduces pre-aging kinetics. The optimal pre-aging temperature and time were consequently found to increase when Sn is added. We also studied the effect of adding a further thermal spike to the usual long-term pre-aging, at different positions within the processing route. The results we present are discussed based on a simulation of vacancy evolution in the alloy when subjected to these treatments.
With the aim of fully exploiting the advantageous strength-to-weight ratio evident in Al-Mg-Si alloys, this study presents measures for increasing the yield strength of an EN AW-6082 type plate alloy. In addition to describing the thermodynamic simulation-based adjustment of age-hardenable elements (Si, Mg and Cu) and a modified artificial ageing treatment, it investigates the effects of adding a small amount of Zr. The significant strengthening induced by adding Zr is correlated with sub-grain boundary hardening in a recovered microstructure after solution annealing at 570°C, compared with the almost entirely recrystallized microstructure in an unmodified EN AW-6082 alloy. In combination with a maximum dissolvable number of age-hardenable elements and interrupted quenching, which comprises an improved heat treatment strategy for thick plates, it is seen that the yield strength can be increased by more than 40% to 411 MPa compared to conventional EN AW-6082 base material as verified by tensile testing. In the study scanning electron microscopy and scanning transmission electron microscopy were performed for microstructural characterization with a focus on particle and deformation analysis. All individual contributions which generated the superior strength are calculated and discussed in order to reveal the microstructure-property relationship.