WO 3 was incorporated into a carbon aerogel with controllable single or hybrid structure, and the latter structure exhibited better capacitive performance.
The deformed microstructures of Ni20Cr wires include amorphous GB, crystal GB, edge dislocations, and twins. Edge dislocations exist in GB and grain interiors. Twinning angles is approximately 141° and 146°, respectively.
Preparation of a size controllable porous polymethylmethacrylate template and Cu micro/nanowire arrays by an iterative melt co-drawing and bundling technique.
24 May 2016 in High Temperature Materials and Processes
Ni80Cr20 (Ni20Cr, wt%) micro-wires were fabricated by the cold-drawing method with single die. Abnormal engineering strains were approximately 17.3–46.6 % for each pass. The relationship between mechanical properties and microstructures of Ni20Cr micro-wires were investigated under different engineering strains and annealing conditions. Experiment results indicate that the as-drawn NiCr micro-wires present obviously brittle fractures. The ultimate tensile strength (UTS) significantly increases from 781 to 1,147 MPa and the elongation decreases from 17.2 % to 1 % with engineering strains increasing. The deformed microstructures of Ni20Cr micro-wire were analyzed in detail including two-phase (solid solution/amorphous phase), edge dislocations and twins. With the annealing temperature increasing, specimens had experienced three stages and their mechanical properties were improved. After annealing at 890 °C (with 6.5 g stress) for 7.3 s in N2, the Ni20Cr micro-wires benefited for the second drawing pass. The results are very importance in fabricating Ni20Cr micro-wire with the diameter from 25 to 10 μm.