The microstructure and corrosion rate of as-cast and heat-treated binary Mg-Ga alloys with gallium content ranging from 0.375 to 1.5 wt. % were investigated. The corrosion rate was determined by the weight loss method using a simulated body fluid (SBF). The microstructure of the as-cast alloys showed an α-Mg matrix of dendritic morphology with intermetallic compounds Mg5Ga2 located mainly at the interdendritic regions. The fraction and size of the Mg5Ga2 particles increased with the amount of Ga in the alloy. The grain size decreased as the Ga content was increased. The products formed on the surface of the Mg-Ga alloys after immersion in SBF were MgO, Mg(OH)2, and calcium phosphates. The corrosion rate of the as-cast alloys was dependent on the Ga content. At concentrations lower than 1 wt. % the corrosion rate was similar to that of pure Mg (0.65 mm/year). However, Ga additions higher than 1 wt. % worsened the corrosion resistance. After heat treatment, the corrosion rate of Mg-Ga alloys decreased, and in the case of the alloys with Ga concentrations lower than 1 wt. %, corrosion rate was lower than that of pure Mg. Corrosion of these alloys after heat treatment was uniform.
7 October 2021 in Journal of Biomedical Materials Research Part B: Applied Biomaterials
The effect of cross- or unidirectional rolling on the microstructure, corrosion rate, texture, and hemolysis of the Mg-0.5Zn-0.25Ga and Mg-1.5Zn-0.375Ga alloys was evaluated. After both rolling processes, the microstructure of the as-cast alloys was considerably refined due to the recrystallization process, obtaining higher grain refinement after cross-rolling. The Mg-1.5Zn-0.375Ga alloy showed a finer microstructure than the Mg-0.5Zn-0.25Mg alloy due to the effect of both the severe plastic deformation obtained after cross-rolling and the higher amount of alloying elements, which act as grain refiners. After unidirectional rolling, the texture intensity of the basal plane increases, while the cross-rolled alloys show lower texture intensity due to the activation of the pyramidal and/or prismatic slip systems. The cross-rolled alloys showed a higher corrosion rate than the unidirectionally rolled alloys due to the basal texture developed. The Mg-1.5Zn-0.375Ga alloy showed a higher corrosion rate than the Mg-0.5Zn-0.25Ga alloy since the voids formed during heat treating were not fully eliminated during rolling. The Mg-0.5Zn-0.25Ga alloy after unidirectional rolling was not hemolytic (4.7%) and showed the lowest corrosion rate (0.8 mm/y). Thus, this alloy may be an excellent candidate for use in the fabrication of biodegradable implants.