Single walled carbon nanotubes (SWCNTs) are used as a component of a plating solution of CuSO4 for direct current electrodeposition of Cu–SWCNT composites with varying nanotube proportions without the use of either a surfactant, a dispersing agent, or functionalization of the SWCNTs. The Cu–SWCNT composites are characterized by scanning electron microscopy (SEM), energy dispersive X-ray analysis (EDX), X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), and Raman spectroscopy. The composites are comprised of metallic Cu and SWCNTs with minor oxide impurities, as well as the residual (Fe) catalyst from the unpurified SWCNTs, in addition to displaying nanotube-mediated morphological differences. EDX analysis of carbon (wt%) is close to quantitative with respect to the wt% of SWCNTs added to the electrolysis solution. The presence of SWCNTs decreases the oxidation of the copper, as well as changing the identity of the oxide from CuO, for electrolysis of Cu, to Cu2O. Hard adherent Cu–SWCNT coatings are prepared by the addition of Cu powder to the electrolysis solution. The approach described in this paper will enable controlled synthesis of metal-nanomaterial composites that can potentially be processed further into high ampacity electrical conductors.
The growth of carbon nanotubes (CNTs) by direct liquid injection chemical vapor deposition (DLICVD) has been studied using the polyoxometalate cluster [HxPMo12O40⊂H4Mo72Fe30(O2CMe)15O254(H2O)98-y(EtOH)y] (FeMoC) as the catalyst with either ethanol or toluene as the carbon source. In order to screen different growth conditions a single large batch of FeMoC is required in order to eliminate variation in the catalyst precursor. The preparation of 6 g of FeMoC is possible by scaling (10×) literature reagent ratios. DLICVD studies of the FeMoC derived carbon product were evaluated by Raman spectroscopy and scanning electron microscopy (SEM) to determine the quality (G:D ratio) and purity of CNT content. With the use of ethanol as the carbon source, increasing the temperature in the injection zone (aspiration temperature) above 250 °C increases the yield, and results in a slight increase in the G:D ratio. The maximum yield is obtained with a growth temperature of 900 °C, while the G:D ratio is the highest at higher temperatures. Faster solution injection rates increase yield, but with a significant decrease in G:D, in fact no CNTs are observed in the product for the highest injection rate (10 mL/h). An optimum catalyst concentration of 1.25 wt.% is found, which influences both the catalyst:C and catalyst:H ratios within the system. Growth at 800 °C is far more efficient for toluene as a carbon source than ethanol. The resulting “process map” allows for large quantities of CNTs to be prepared by DLICVD.
The electromigration behaviour of raw and acid purified single walled carbon nanotubes (SWCNTs) in dilute aqueous systems (0.0034 mg mL−1), in the absence of surfactant, with the addition of either 0.85 M acetic acid or 0.1 M CuSO4, was evaluated using a 2-inch copper cathode and either a 2-inch copper or 0.5-inch platinum anode. The results showed that the electromigration of raw SWCNTs (with a high catalyst residue) in the presence of CuSO4 resulted in the formation of a Cu-SWCNT composite material at the cathode. In contrast, acid purified SWCNTs were observed to diffuse to a copper anode, creating fibrillated agglomerates with “rice-grain”-like morphologies. Upon acidification with acetic acid (or addition of CuSO4) the direction of electromigration reversed towards the cathode as a result of coordination of Cu2+ to the functional groups on the SWCNT overcoming the inherent negative charge of the acid purified SWCNTs. The result was the co-deposition of SWCNTs and Cu metal on the cathode. Addition of 0.005 M EDTA sequesters some of the Cu2+ and resulted in the separation of metal decorated SWCNTs to the cathode and un-decorated SWCNTs to the anode. The resulting SWCNT and Cu/SWCNT deposits were characterized by Raman spectroscopy, XPS, SEM, EDS, and TEM.
In this work, as-received HiPCO single walled carbon nanotubes (SWCNTs) are incorporated in a controllable manner at various concentrations into Cu-SWCNT composites via electroless plating, by varying the related reaction times, with polyethylene glycol (PEG) used as a dispersing agent. The resultant samples were analyzed using scanning electron microscopy (SEM) for morphology assessment, energy dispersive X-ray analysis (EDX) and X-ray photoelectron spectroscopy (XPS) for elemental analysis, X-ray diffraction (XRD) for the assessment of crystal phase identification, and Raman spectroscopy for the confirmation of the presence of the incorporated SWCNTs. The Cu-SWCNT composites were found to contain carbon, catalytic iron (associated with the raw, as-received SWCNTs), oxygen, and copper; the latter was found to be inversely proportional to carbon and iron contents. The oxygen (associated with both the SWCNT defect sites and oxidized copper surfaces) remained more or less constant regardless of the proportion of SWCNTs in the composites. The Raman IG:ID ratio remains within the experimental error constant, indicating that the electroless deposition does not have a deleterious effect on the SWCNTs. At short deposition times, SEM revealed a relatively dense structure comprising a distinctive fibrous morphology, suggestive of an underlying SWCNT substrate coated with copper; however, with increasing deposition, a more porous morphology is observed. The size of the granular particles increases up until 10 min of reaction, after which time it remains unchanged.
Herein, we report the successful use of newspaper as a substrate for the growth of single-walled carbon nanotubes (SWCNTs) by chemical vapor deposition (CVD) with intriguing results demonstrating that (a) the large surface area of newspaper stock allows for SWCNT growth and (b) only newspaper produced with kaolin clay sizing allowed for SWCNT growth. Kaolin newsprint was impregnated with Al2O3 and Fe(NO3)3·9H2O (as precursors to FexOy nanoparticles), and calcined (30 min at 400 °C). The subsequent char residue was loaded into a CVD chamber and used as a substrate for SWCNT growth at 750 °C, using H2, C2H2, and water vapor as the growth gas. Samples of raw carbon soot exhibiting fluorescence spectra, indicative of SWCNTs, were further evaluated by resonant Raman spectroscopy, and by transmission electron microscopy (TEM). The calcinated substrate remnants were evaluated by scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS). Experiments utilizing paper substrates produced with kaolin filler resulted in hybridized sp2–sp3 bonded carbon species. The soot was found to consist primarily of carbon nanotubes and bi-layer graphene in the form of collapsed nanotubes, also known as graphene nanoribbons (GNR).
The increasing availability of the user-friendly black box can present an increased probability of characterization errors. The uninformed choice (e.g., any SEM will see this) or dependence on one instrument can also lead to erroneous results. Failure to understand the limits and advantages of a particular instrument and bias through assumption or desired result can be equally deceptive. In the example presented here, the objectives are to determine primary particle size and to identify the impurities in a specimen. We will look at the data produced by several instruments and discuss the ways each technology can support or mislead the analysts. Images were acquired optically by secondary electron (SE), x-ray dot maps and back scattering electrons (BSE). The elemental analysis techniques used were Energy Dispersive Spectrometry (EDS), Wavelength Dispersive Spectrometry (WDS) and Powder x-ray diffractometry (PXD). Field emission SEM (FESEM) and optical images are used.