To commercialize the technology of photoelectrochemical hydrogen production, it is essential to surpass the US. Department of Energy target of 0.36 mmol h−1 cm−2 for 1-sun hydrogen production rate. In this study, we utilize crystalline silicon, which can exhibit the highest photocurrent density (43.37 mA cm−2), as the photoelectrode material. However, achieving bias-free water splitting (>1.6 V) remains challenging due to the intrinsic low photovoltage of crystalline silicon (0.6 V). To address this limitation, we replace water oxidation with low-potential furfural oxidation, enabling not only bias-free hydrogen production but also dual hydrogen production at both the cathodic and anodic sides. This approach results in a record 1-sun hydrogen production rate of 1.40 mmol h−1 cm−2, exceeding the Department of Energy target by more than fourfold.
Pd-based catalysts are widely used in the oxidation of CH4 and have a significant impact on global warming. However, understanding their active sites remains controversial, because interconversion between Pd and PdO occurs consecutively during the reaction. Understanding the intrinsic active sites under reaction conditions is critical for developing highly active and selective catalysts. In this study, we demonstrated that partially oxidized palladium (PdOx) on the surface plays an important role for CH4 oxidation. Regardless of whether the initial state of Pd corresponds to oxides or metallic clusters, the topmost surface is PdOx, which is formed during CH4 oxidation. A quantitative analysis using CO titration, diffuse reflectance infrared Fourier-transform spectroscopy, X-ray diffraction, and scanning transmission electron microscopy demonstrated that a surface PdO layer was formed on top of the metallic Pd clusters during the CH4 oxidation reaction. Furthermore, the time-on-stream test of CH4 oxidation revealed that the presence of the PdO layer on top of the metallic Pd clusters improves the catalytic activity. Our periodic density functional theory (DFT) calculations with a PdOx slab and nanoparticle models aided the elucidation of the structure of the experimental PdO particles, as well as the experimental C-O bands. The DFT results also revealed the formation of a PdO layer on the metallic Pd clusters. This study helps achieve a fundamental understanding of the active sites of Pd and PdO for CH4 oxidation and provides insights into the development of active and durable Pd-based catalysts through molecular-level design.
11 April 2023 in The Journal of Physical Chemistry C
Ethylene can be synthesized in a renewable manner by dehydrating bioethanol over supported metal oxide nanoparticle catalysts. Here, a series of nanoparticulate tungsten oxides supported on MFI (Mobil five) zeolite nanosheets was prepared at different W loadings (1 to 6 mol %) using the incipient wetness method and investigated with respect to the ability to catalyze the dehydration of ethanol. The resulting samples were characterized by X-ray diffraction, electron microscopy, N2 isotherms, X-ray absorption fine structures, and by the temperature-programmed desorption of NH3. The results obtained showed that WOx nanoparticles were homogeneously distributed over the entire void space of nanosheet samples up to a loading of 2 mol %, after which large WOx nanoparticles with needle-like morphology were formed on the surface of the zeolite nanosheet beyond 2mol%. The number of acid sites increased with WOx loading and, as a result, EtOH conversion progressively increased with WOx loading up to 6 mol %. At reaction temperatures of >390 °C, homogeneously distributed WOx nanoparticles showed slightly higher ethylene selectivity than nano-needle structured WOx. However, nano-needle structured WOx exhibited greater catalytic stability. In terms of ethylene yield over 8 h, needle-like WOx nanoparticles were found to be more suitable for the acid-catalyzed dehydration of ethanol than small-sized WOx nanoparticles.