Liquid crystals (LCs) represent one of the foundations of modern communication and photonic technologies. Present display technologies are based mainly on nematic LCs, which suffer from limited response time for use in active colour sequential displays and limited image grey scale. Herein we report the first observation of a spontaneously formed helix in a polar tilted smectic LC phase (SmC phase) of achiral bent-core (BC) molecules with the axis of helix lying parallel to the layer normal and a pitch much shorter than the optical wavelength. This new phase shows fast (∼30 μs) grey-scale switching due to the deformation of the helix by the electric field. Even more importantly, defect-free alignment is easily achieved for the first time for a BC mesogen, thus providing potential use in large-scale devices with fast linear and thresholdless electro-optical response.
The characteristics of the twist-bend nematic (NTB) phase of an achiral asymmetrical rigid bent-core liquid crystal (LC), the ends of which are terminated by symmetric alkyl chains, are reported. The nematic–nematic phase transition and its properties are studied by differential scanning calorimetry (DSC), polarising microscopy and the electro-optic techniques. Large domains of opposite handedness are observed in the absence of the external field in the NTB phase. Another set of periodic striped pattern consisting of domains with sharp boundaries is formed when a high-frequency electric field with a magnitude above its threshold is applied across a planarly aligned cell. The neighbouring domains are of opposite chirality. The temperature dependence of the heliconical angle θ0 is determined from the birefringence measurements using Haller’s extrapolation technique. This material shows lower values of the heliconical angle (~9.3° at a temperature of 155°C within the NTB phase) when compared with the previously reported dimer-based twist-bend nematic LCs (31°±3°). GRAPHICAL ABSTRACT
12 March 2021 in The International Journal of Advanced Manufacturing Technology
Food spoilage is an ongoing global issue that contributes to rising carbon dioxide emissions and increased demand for food processing. This work developed anti-bacterial coatings utilising inkjet printing of silver nano-inks onto food-grade polymer packaging, with the potential to enhance food safety and reduce food spoilage. Silver nano-inks were synthesised via laser ablation synthesis in solution (LaSiS) and ultrasound pyrolysis (USP). The silver nanoparticles (AgNPs) produced using LaSiS and USP were characterised using transmission electron microscopy (TEM), Fourier transform infrared (FTIR) spectroscopy, UV-Vis spectrophotometry and dynamic light scattering (DLS) analysis. The laser ablation technique, operated under recirculation mode, produced nanoparticles with a small size distribution with an average diameter ranging from 7–30 nm. Silver nano-ink was synthesised by blending isopropanol with nanoparticles dispersed in deionised water. The silver nano-inks were printed on plasma-cleaned cyclo-olefin polymer. Irrespective of the production methods, all silver nanoparticles exhibited strong antibacterial activity against E. coli with a zone of inhibition exceeding 6 mm. Furthermore, silver nano-inks printed cyclo-olefin polymer reduced the bacterial cell population from 1235 (±45) × 106 cell/mL to 960 (±110) × 106 cell/mL. The bactericidal performance of silver-coated polymer was comparable to that of the penicillin-coated polymer, wherein a reduction in bacterial population from 1235 (±45) × 106 cell/mL to 830 (±70) × 106 cell/mL was observed. Finally, the ecotoxicity of the silver nano-ink printed cyclo-olefin polymer was tested with daphniids, a species of water flea, to simulate the release of coated packaging into a freshwater environment.
25 April 2018 in Beilstein Journal of Nanotechnology
Two homologue achiral bent-core liquid crystals (LCs), BCN66 and BCN84, in their nematic phases are studied by dielectric spectroscopy in the frequency range 10 Hz–10 MHz. In each of these compounds, two relaxation processes are identified and assigned to (i) collective dynamics of molecules in nanometer-sized cybotactic clusters and (ii) individual molecular relaxations, in the ascending order of frequency of the probe field. The temperature and the bias electric field dependence of the dielectric strength and relaxation frequency for these processes are shown to give rise to sharpness in cluster boundaries, increased size and volume fraction in the LC nematic phase. The effect of the bias field on the LC cell is similar to reducing its temperature; both variables increase the cluster size and volume fraction and give rise to sharp cluster boundaries. The findings confirm that dielectric spectroscopy is a powerful and an extremely useful technique to provide a deeper understanding of the mechanism of cybotactic cluster formation in the isotropic liquid and the nematic phase of LCs as a function of temperature and the bias field.
The flexoelectric polarization of four bent-core nematic liquid crystals (LCs) has been measured using the pyroelectric effect. Hybrid aligned nematic cells are fabricated for measuring the pyroelectric response over the entire range of the nematic phase. It is found that the magnitude of flexoelectric polarization and the sum of the flexoelectric coefficients for the bent-core LCs studied here are three to six times higher than for the calamitics. is found to depend on the transverse dipole moment of LC molecules. However, values are by no means giant as alone had been reported for a bent-core nematic system previously. The dependence of the sum of “splay and bend flexoelectric coefficients” is discussed in terms of the shape of the molecule and of the dipole moment directed normal to the molecular axis.