In this paper, a multi-layer and multi-track finite element model of 24CrNiMo alloy steel by selective laser melting (SLM) is established by using the ABAQUS software. The distribution and evolution of temperature field and stress field and the influence of process parameters on them are systematically studied. The results show that the peak temperature increases from 2153 °C to 3105 °C and the residual stress increases from 335 MPa to 364 MPa with increasing laser power from 200 W to 300 W; the peak temperature decreases from 2905 °C to 2405 °C and the residual stress increases from 327 MPa to 363 MPa with increasing scanning speed from 150 mm/s to 250 mm/s; the peak temperature increases from 2621 °C to 2914 °C and the residual stress decreases from 354 MPa to 300 MPa with increasing preheating temperature from 25 °C to 400 °C. Far away from scanning area, far away from starting point, and the adjacent areas with vertical scanning direction, resulting in a uniform temperature distribution, help to reduce the residual stress. Due to the remelting effect, the interlayer scanning angle changing helps to release the residual stress of the former layer causing a smaller residual stress after redistribution.
In this study, the effects of laser volumetric energy density (η) on the metallurgical defect behavior and microstructure evolution of H13 die steel fabricated by selective laser melting (SLM) additive manufacturing are systematically studied, and underlying thermal mechanisms are revealed. The results indicate that the metallurgical defect behavior is significantly affected by the applied η, which is controlled by laser power P and scanning speed v. With increasing P or decreasing v, η increases, the metallurgical defects such as pores and poor fusion initially decrease and then increase, and the density initially increases and then decreases. The typical microstructures induced by SLM are columnar dendrites and equiaxed dendrites. Their growth direction, distribution, and size at different positions in the molten pool are quite different. The size of the columnar crystals with directional full growth is highly correlated with the applied η. As the applied η increases, the length and diameter of the columnar crystals increase, but grains with nonuniform distribution are obtained under a higher η of 122.22 J mm−3. Under the optimized η of 111.11 J mm−3 (P = 200 W, v = 1000 mm/s), the H13 die steel samples fabricated by SLM are near-fully dense and have almost no metallurgical defects (the density reaches 99.13%), and the dense columnar crystals with uniform distribution are obtained. This study may provide a theoretical and experimental basis for the design and optimization of SLM processing parameters and the reliable fabrication of SLM-processed parts with controlled defects and microstructures.
22 March 2019 in IOP Conference Series: Materials Science and Engineering
Laser shock peening is a new and high technology with application value and development prospect. It can effectively improve the fatigue resistance, wear resistance and corrosion resistance of metal materials. In this paper, two-phase titanium alloy TC17, which is widely used in aerospace field, is studied by finite element method. The effects of different laser shock paths on the deformation and residual stress distribution of materials are studied. The results show that the large-area complex path strategy laser shock peening has a certain influence on the deformation and residual stress of TC17. Single-sided, double-sided simultaneous and double-sided non-simultaneous laser shock peening have a great influence on the residual stress size and distribution. Reciprocating path laser shock peening provides less distortion and higher residual stress than a zigzag path.
1 December 2019 in IOP Conference Series: Materials Science and Engineering
In this paper, the finite element analysis model of camshaft for nuclear emergency diesel engine with initial crack defect is established based on ABAQUS finite element analysis software. The effects of initial crack defect parameters on crack tip stress intensity factor are studied by a working condition discretization method. The numerical results show that the crack tip stress intensity factors of transverse crack and longitudinal crack are quite different in a load cycle of camshaft. The crack tip stress intensity factors of transverse crack fluctuate greatly, and the crack tip stress intensity factor range is much larger than that of longitudinal crack, which indicates that the fatigue fracture risk of transverse crack on the camshaft journal is higher. With the increase of initial crack depth from 1 mm to 4 mm, the crack tip stress intensity factor range increases from 410.84 MPa·mm1/2 to 720.24 MPa·mm1/2 by 75.3%, which indicates that the increase of initial crack depth can lead to a significant increase of the fatigue fracture risk. As the initial crack defect moves away from the cam, the maximum of the crack tip stress intensity factor initially increases and then decreases after reaching a maximum value. When the initial crack is 3 mm away from the end face of the cam, the crack tip stress intensity factor range is the largest (843.98 MPa·mm1/2), which indicates that the fatigue fracture risk of transverse crack at this position is the highest. The research results obtained in this paper may provide some reference for the fracture assessment and reliability analysis of camshaft for nuclear emergency diesel engine.
1 December 2019 in IOP Conference Series: Materials Science and Engineering
The hydrogen supply system is the energy supply of hydrogen-powered vehicle. The failure of most parts in the hydrogen supply system is due to the impact and vibration caused by complex road conditions. Therefore, it is required that the hydrogen supply system should have good impact and vibration resistance. In this paper, the Design Exploration module in ANSYS Workbench is used to study the multi-objective optimization about the stiffness and strength of a two-bottle horizontal hydrogen supply system under impact and vibration conditions. The responding surface between the width and length of the frame and the stiffness and strength of the system under different conditions is developed. The optimal frame size which can effectively reduce the stress state of the system structure under impact and vibration condition is obtained.