Jun Wang

Prof. Jun Wang

orcid

Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
8 June 2021 in RSC Advances
Verified
Journal Article
Open access
PDF file
ZRZechun Ren
Zechun Ren
RGRui Guo
Rui Guo
XZXinyuan Zhou
Xinyuan Zhou
HBHongjie Bi
Hongjie Bi
XJXin Jia
Xin Jia
ZHZhenhua Huang
Zhenhua Huang
Molecular details of the combination of degradable material polylactic acid and cellulose.

8 August 2020 in Materials
Verified
Journal Article
Open access
PDF file
BCBin Chen
Bin Chen
JWJun Wang
Jun Wang
JZJinyou Zhao
Jinyou Zhao
The shrinkage of alkali-activated slag (AAS) is obviously higher than ordinary Portland cement, which limited its application in engineering. In this study, the effects of NaAlO2 in mitigating drying shrinkage and autogenous shrinkage of AAS were studied. To further understand the shrinkage mechanism, the hydration products and microstructures were studied by X-ray diffraction, scanning electron microscopy and nitrogen adsorption approaches. As the partial substitution rate of NaAlO2 for Na2SiO3 increased, the drying shrinkage and autogenous shrinkage reduced significantly. The addition of NaAlO2 could slow down the rate of hydration reaction and reduce the porosity, change the pore diameter and the composition of generated paste and cause more hydrotalcite and tetranatrolite generated—which contributed to reduced shrinkage. Additionally, raising the Na2O content rate caused obvious differences in drying shrinkage and autogenous shrinkage. As the Na2O content elevated, the drying shrinkage decreased and autogenous shrinkage increased. A high Na2O content would cause complete hydration reactions and provoke high autogenous shrinkage. However, incomplete hydration reactions left more water in the paste, and the evaporated water dramatically influenced drying shrinkage. The results indicate that addition of NaAlO2 could greatly mitigate the drying shrinkage and autogenous shrinkage of AAS.

3 January 2022 in Materials
Verified
Journal Article
Open access
PDF file
JWJun Wang
Jun Wang
XWXinran Wang
Xinran Wang
XDXin Yu Duan
Xin Yu Duan
YSYu Su
Yu Su
XYXinyu Yi
Xinyu Yi
At present, the existing standards (AISC360-16, EN1994-1-1:2004, and JGJ138-2016) lack relevant provisions for steel-reinforced concrete (SRC) composite columns with high-strength steel. To investigate the axial compressive mechanical performance of short high-strength steel-reinforced concrete (HSSRC) columns, the axial load test was conducted on 12 short composite columns with high-strength steel and ordinary steel. The influences of steel strength, steel ratio, and the section form of steel on the failure modes, bearing capacity, and ductility of the specimens were studied. Afterward, the experimental data were compared with the existing calculation results. The results show: compared with the specimens with Q235 steel, the bearing capacity of the specimens with Q460 steel increases by 7.8–15.3%, the bearing capacity of the specimens with Q690 steel increases by 13.2–24.1%, but the ductility coefficient increases by 15.2–202.4%; with the increase of steel ratio, the bearing capacity and ductility of specimens are significantly improved. A change of the steel cross-section could influence the ductility of SRC columns more than their bearing capacity. Moreover, the calculation results show that present standards could not predict the bearing capacity of HSSRC columns. Therefore, a modified method for determining the effective strength of steel equipped in HSSRC columns was proposed. The results of the ABAQUS simulation also showed that the addition of steel fibers could significantly improve the bearing capacity of Q690 HSSRC columns. The research results provide a reference for engineering practices.

1 January 2021 in Advances in Materials Science and Engineering
Verified
Journal Article
Open access
PDF file
BCBin Chen
Bin Chen
JWJun Wang
Jun Wang
A freeze‐thaw resistance is an important indicator of the durability of alkali‐activated slag concrete, which causes structural failure when the performance is low, especially in severely cold areas. In this study, solid sodium aluminate and sodium silicate were used as composite alkaline activators, while slag was used as the raw material to prepare alkali‐activated slag concrete, whose freeze‐thaw resistance, as well as that of ordinary cement concrete, was experimentally studied by varying the freeze‐thaw cycles. The effects of the mass, compressive strength, and dynamic elastic modulus of the sample were investigated by considering the influence of different water‐to‐slag ratios and slag contents, while the damage variables and model were also analyzed. The results showed that alkali‐activated slag concrete had an excellent freeze‐thaw resistance, which was significantly affected by the water‐to‐slag ratio and compressive strength; specifically, the higher the water‐to‐slag ratio, the lower the freeze‐thaw resistance, and the higher the compressive strength, the better the freeze‐thaw resistance. The freeze‐thaw durability, microstructure, and damage mechanism were studied via microscopic analysis. When analyzed via the microstructure test, crack pores and microcracks with narrow spaces and large surface areas were generated under freeze‐thaw damage conditions, but the dense hydration structure and high‐bonding‐strength hydration products led to a better freeze‐thaw resistance. The damage model was established using compressive strength and relative dynamic elastic modulus as damage variables, and the attenuation exponential and accumulative damage power function model had a high accuracy, which could better reflect the freeze‐thaw damage law and damage degree and predict the lifetime of alkali‐activated slag concrete.

19 April 2022 in Materials
Verified
Journal Article
Open access
PDF file
JWJun Wang
Jun Wang
XYXinyu Yi
Xinyu Yi
QLQi Liu
Qi Liu
XFXueqi Fang
Xueqi Fang
In this paper, based on the low-cycle loading tests of 11 steel-reinforced concrete (SRC) frame columns with built-in Q690 steel and 5 SRC frame columns with built-in Q235 steel, a systematic study on their seismic performance was carried out. The design parameters of the specimens were the steel strength, axial compression ratio, shear span ratio, steel content, and stirrup ratio. The failure modes, stress characteristics, hysteresis curve, skeleton curve, displacement ductility performance, energy dissipation capacity, and other main seismic indicators of the specimens with different parameters were analyzed, and the corresponding relationship between the displacement ductility performance of the specimen and the energy dissipation capacity and design parameters was obtained. The results show that the load–displacement curve of the specimens is relatively full, the descending section is gentle, and various seismic performance indicators are relatively excellent, reflecting good seismic performance. Equipped with high-strength steel SRC frame columns, they can better bear the horizontal load, the displacement ductility performance is improved, and the energy dissipation capacity is slightly lower than that of ordinary-strength steel SRC frame columns. The increase in the shear span ratio, steel content, and stirrup ratio of the specimens helps to improve their seismic performance, whereas an increase in the axial compression ratio makes their seismic performance worse.

14 November 2021 in Materials
Verified
Journal Article
Open access
PDF file
JWJun Wang
Jun Wang
XDXin Yu Duan
Xin Yu Duan
YWYifan Wang
Yifan Wang
XWXinran Wang
Xinran Wang
QLQi Liu
Qi Liu
To investigate the applicability of the methods for calculating the bearing capacity of high-strength steel-reinforced concrete (SRC) composite columns according to specifications and the effect of confinement of stirrups and steel on the bearing capacity of SRC columns. The axial compression tests were conducted on 10 high-strength SRC columns and 4 ordinary SRC columns. The influences of the steel strength grade, the steel ratio, the types of stirrups and slenderness ratio on the bearing capacity of such members were examined. The analysis results indicate that using high-strength steel and improving the steel ratio can significantly enhance the bearing capacity of the SRC columns. When the slenderness ratio increases dramatically, the bearing capacity of the SRC columns plummets. As the confinement effect of the stirrups on the concrete improves, the utilization ratio of the high-strength steel in the SRC columns increases. Furthermore, the results calculated by AISC360-19(U.S.), EN1994-1-1-2004 (Europe), and JGJ138-2016(China) are too conservative compared with test results. Finally, a modified formula for calculating the bearing capacity of the SRC columns is proposed based on the confinement effect of the stirrups and steel on concrete. The results calculated by the modified formula and the finite element modeling results based on the confinement effect agree well with the test results.