Photocatalytic utilization of CO2 in the production of value-added chemicals has presented a recent green alternative for CO2 fixation. In this regard, three FeNbO4/NH2-MIL-125(Ti) composites of different mole ratios were synthesized, characterized using Powder X-ray diffraction (PXRD), UV–vis diffuse reflectance spectroscopy (UV-Vis DRS), Brunauer–Emmett–Teller (BET), Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray (EDX). PXRD patterns confirm the co-existence of the parent components in the prepared composites. Moreover, the surface area increased as the mole percent of NH2-MIL-125(Ti) in the composites increased due to the large surface area of NH2-MIL-125(Ti). Prepared composites were investigated for the photocatalytic insertion of CO2 into propylene oxide. FeNbO4(75%)/NH2-MIL-125(Ti)(25%) showed the highest percent yield of 52% compared to the other two composites. Results demonstrate the cooperative mechanism between FeNbO4 and NH2-MIL-125(Ti) and that the reaction proceeded photocatalytically.
α- and β-BiNbO4 nanoparticles were successfully prepared using three different routes, namely co-precipitation, hydrothermal, and citrate precursor methods. Structural characterization has been analyzed using powder X-ray diffraction where results confirmed the mixed-phase nature of the prepared powders. When co-precipitation method is applied, BiNbO4 prepared at pH 2 and calcined at 750 °C shows predominately the α-BiNbO4 owning the narrowest band gap of 2.86 eV, whereas an increase in the pH value resulted in the β-BiNbO4 phase being the predominant phase. On the other hand, samples prepared using citrate precursor method show co-existence of both α- and β-BiNbO4 at all pH values under study; however, at pH 10 the β-BiNbO4 was the dominant phase exhibiting a higher bandgap energy value of 3.16 eV. When applying the hydrothermal approach, BiNbO4 prepared at all pH ranges of the present study show a band gap >3.2 eV indicating their activity in the ultraviolet region of the spectrum. Moreover, increasing calcination temperature to 900 °C, a gradual transformation of α- to β was observed. Lastly, it was noticed that as the lattice volume increases, the band gap of prepared BiNbO4 decreases.