State Key Laboratory of Fine Chemicals, Department of Catalytic Chemistry and Engineering, School of Chemical Engineering, Dalian University of Technology, Dalian, China
Prof. Dr. Xinwen Guo
State Key Laboratory of Fine Chemicals, Department of Catalytic Chemistry and Engineering, School of Chemical Engineering, Dalian University of Technology, Dalian, China
Identifying the dynamic structure of heterogeneous catalysts is crucial for the rational design of new ones. In this contribution, the structural evolution of Fe(0) catalysts during CO 2 hydrogenation to hydrocarbons has been investigated by using several (quasi) in situ techniques. Upon initial reduction, Fe species are carburized to Fe 3 C and then to Fe 5 C 2 . The by-product of CO 2 hydrogenation, H 2 O, oxidizes the iron carbide to Fe 3 O 4 . The formation of Fe 3 O 4 @(Fe 5 C 2 +Fe 3 O 4 ) core-shell structure was observed at steady state, and the surface composition depends on the balance of oxidation and carburization, where water plays a key role in the oxidation. The performance of CO 2 hydrogenation was also correlated with the dynamic surface structure. Theoretical calculations and controll experiments reveal the interdependence between the phase transition and reactive environment. We also suggest a practical way to tune the competitive reactions to maintain an Fe 5 C 2 -rich surface for a desired C 2+ productivity.
We present here a simple solvothermal method to fabricate metal–organic framework NH2-MIL-53(Al) crystals with controllable size and morphology just by altering the ratio of water in the DMF–water mixed solvent system without the addition of any surfactants or capping agents. With increasing the volume ratio of water in the mixed solvents, a series of NH2-MIL-53(Al) crystals with different sizes and morphologies were synthesized. The average size of the smallest crystal is 76 ± 20 nm, which provides us a simple and environmentally friendly way to prepare nanoscale MOFs. The largest BET surface area of these samples is 1882 m2 g−1 that is mainly contributed by its micropore surface area, and its corresponding micropore volume is 0.83 cm3 g−1, which have greatly extended its application in the fields of gas adsorption and postsynthetic modification. All these samples were characterized by SEM, XRD, N2 adsorption/desorption, TGA and FT-IR. Then a mechanism for the impact of the water ratio on the crystal size and morphology is presented and discussed.