This study demonstrates an efficient method for the synthesis of thermoreversible cross-linked ethylene/propylene rubbers (EPRs) via two steps; in the first step, a functional olefin monomer containing a furan group (FO) is designed and the ethylene/propylene/FO terpolymerization catalyzed by a traditional Ziegler–Natta catalyst is implemented; in the second step, a cross-linked network is constructed via Diels–Alder (DA) click reaction between the bismaleimide and pendant furan groups in the EPR chains. Via polymerization, the FO content in the copolymers was tailored in relatively wide range from 1.1 mol% to 9.7 mol%; this provided various cross-linking precursory groups for the DA reaction. Moreover, the cross-linking density could be adjusted via not only the amount of the inserted furan group but also the ratio of furan to bismaleimide. These solid thermoreversibile EP rubbers could perform their de-cross-linking above 110 °C and re-form the network below 85 °C in a heating–cooling cycle not only in the static measurement of FTIR, but also in the dynamic test of DMA. The mechanical properties of the resulting products with varied cross-linking densities were compared with that of the non-cross-linked polymer and proved to be of much higher modulus. This thermoreversible cross-linking behavior also provided a new strategy for local-repairing of any crack in rubber products.
With neighboring group participation, polypropylene-based transesterification covalent adaptable networks were facilely prepared via the reaction of maleic anhydride grafted polypropylene and diol without using external catalysts.
Designing reversibly cross-linked polymer materials is of great importance for repeated processing. In this work, a Diels–Alder (DA) reaction between furan and maleimide was utilized to achieve thermoreversible cross-linking of ethylene/propylene rubber (EPR) by first constructing EPR with furyl pendent groups and then adding bismaleimide molecules as a cross-linking agent. The kinetics of the cross-linking reaction was detected using the rheological test, and the apparent kinetic rate coefficient (kCL) and Arrhenius activation energy (Ea, CL) of the cross-linking reaction were determined. By adjusting the furyl content of EPR and the molecular structure of the bismaleimide, the influence of the furan/maleimide ratio as well as the bismaleimide structure on the Ea, CL value was investigated, which might provide support for the efficient realization of reversible cross-linking in polymers and the repeated processing of materials via DA chemistry.
A series of elastomeric hydrogels with repeated processability were prepared in this work. These hydrogels were obtained by cross-linking of two common polymers, poly(ethylene-co-propylene) (ethylene-propylene rubber, EPR) and poly(ethylene glycol) (PEG), via dynamic covalent bonds, specifically, through firstly furyl functionalization of EPR at the side groups and maleimide modification of PEG at the chain ends, and followed by the Diels–Alder reaction between furan and maleimide to construct thermoreversible EPR–PEG networks. The composition and microstructure of the network were adjustable in a wide range by facilely tuning the PEG feeding ratios and molecular weights (as the cross-linking agent). In the network the crystalline PEG and the elastic EPR endowed the material with strength and toughness respectively in the dry state, giving a fracture strength of 4–6 MPa and elongation at break of up to 380%; meanwhile, due to the hydrophilicity of PEG, the network could absorb water and form hydrogels, in which the hydrophobic EPR elastomer enhanced the hydrogels effectively. By tailoring the amount and the chain structure of the PEG moiety, the water absorption of the copolymer could reach as high as 356% in 1 hour, and the hydrogel elongation at break could achieve ∼400%, which was comparable to that of pristine cross-linked EPR. The material displayed low cytotoxicity in MC3T3-L1 cells and was biocompatible.
The Diels–Alder (D–A) reaction between furan and maleimide is a thermally reversible reaction that has become a vital chemical technique for designing polymer structures and functions. The kinetics of this reaction, particularly in polymer bulk states, have significant practical implications. In this study, we investigated the feasibility of utilizing infrared spectroscopy to measure the D–A reaction kinetics in bulk-state polymer. Specifically, we synthesized furan-functionalized polystyrene and added a maleimide small-molecule compound to form a D–A adduct. The intensity of the characteristic absorption peak of the D–A adduct was quantitatively measured by infrared spectroscopy, and the dependence of conversion of the D–A reaction on time was obtained at different temperatures. Subsequently, the D–A reaction apparent kinetic coefficient kapp and the Arrhenius activation energy Ea,D–A were calculated. These results were compared with those determined from 1H-NMR in the polymer solution states.