The role of microstructural damage in controlling the edge stretchability of Complex-Phase (CP) and Dual-Phase (DP) steels was evaluated using hole tension experiments. The experiments considered a tensile specimen with a hole at the center of specimen that is either sheared (sheared edge condition) or drilled and then reamed (reamed edge condition). The damage mechanism and accumulation in the CP and DP steels were systematically characterized by interrupting the hole tension tests at different strain levels using scanning electron microscope (SEM) analysis and optical microscopy. Martensite cracking and decohesion of ferrite-martensite interfaces are the dominant nucleation mechanisms in the DP780. The primary source of void nucleation in the CP800 is nucleation at TiN particles, with secondary void formation at martensite/bainite interfaces near the failure strain. The rate of damage evolution is considerably higher for the sheared edge in contrast with the reamed edge since the shearing process alters the microstructure in the shear affected zone (SAZ) by introducing work-hardening and initial damage behind the sheared edge. The CP microstructures were shown to be less prone to shear-induced damage than the DP materials resulting in much higher sheared edge formability. Microstructural damage in the CP and DP steels was characterized to understand the interaction between microstructure, damage evolution and edge formability during edge stretching. An analytical model for void evolution and coalescence was developed and applied to predict the damage rate in these rather diverse microstructures.
27 September 2017 in Journal of Physics: Conference Series
The VDA238-100 standard for tight radius bending (v-bending) of sheet materials has received widespread acceptance with automotive suppliers and material producers to characterize local formability. However, the test fixture and tooling in the v-bend test standard is not amenable to direct strain measurement and the operator cannot terminate the test at the onset of crack initiation as the outer bend surface is not visible. Consequently, fracture is identified using a load threshold and the bend angle estimated from an analytical formula based upon the punch displacement and tooling geometry. Bend angles are not directly transferable and must be interpreted relative to the sheet thickness and bend radius unlike a strain measurement. By obtaining an in-situ strain measurement on the surface using digital image correlation (DIC), the plane strain fracture limit can be accurately identified at the onset of cracking and remove ambiguity in translating the bend angles to practical forming operations and simulations. A novel inverted VDA test frame was developed to incorporate DIC strain measurement during the bend test and a variety of advanced high strength sheet materials were evaluated. It was observed that the VDA bend test creates a homogeneous strain state of plane strain across the width of the sample along with a proportional strain path to fracture without necking that is ideal for fracture characterization. A correlation is developed to relate the bend angle with the major strain for the materials considered and accounts for the sheet thickness and bend radius. A comparison of the bend angle obtained using the formula in the VDA standard based on the punch displacement was in very good agreement with manual measurements and an algorithm to measure the bend angle using DIC analysis was developed.
While the third generation of advanced high-strength steels (3rd Gen AHSS) have increasingly gained attention for automotive lightweighting, it remains unclear to what extent the developed methodologies for the conventional dual-phase (DP) steels are applicable to this new class of steels. The present paper provides a comprehensive study on the constitutive, formability, tribology, and fracture behavior of three commercial 3rd Gen AHSS with an ultimate strength level ranging from 980 to 1180 MPa which are contrasted with two DP steels of the same strength levels and the 590R AHSS. The hardening response to large strain levels was determined experimentally using tensile and shear tests and then evaluated in 3D simulations of tensile tests. In general, the strain rate sensitivity of the two 3rd Gen 1180 AHSS was significantly different as one grade exhibited larger transformation-induced behavior. The in-plane formability of the three 1180 MPa steels was similar but with a stark contrast in the local formability whereas the opposite trend was observed for the 3rd Gen 980 and the DP980 steel. The forming limit curves could be accurately predicted using the experimentally measured hardening behavior and the deterministic modified Bressan–Williams through-thickness shear model or the linearized Modified Maximum Force Criterion. The resistance to sliding of the three 3rd Gen AHSS in the Twist Compression Test revealed a comparable coefficient of friction to the 590R except for the electro-galvanized 3rd Gen 1180 V1. An efficient experimental approach to fracture characterization for AHSS was developed that exploits tool contact and bending to obtain fracture strains on the surface of the specimen by suppressing necking. Miniature conical hole expansion, biaxial punch tests, and the VDA 238-100 bend test were performed to construct stress-state dependent fracture loci for use in forming and crash simulations. It is demonstrated that, the 3rd Gen 1180 V2 can potentially replace the DP980 steel in terms of both the global and local formability.
Magnesium sheet metal alloys have a hexagonal close packed (hcp) crystal structure that leads to severe evolving anisotropy and tension-compression asymmetry as a result of the activation of different deformation mechanisms (slip and twinning) that are extremely challenging to model numerically. The low density of magnesium alloys and their high specific strength relative to steel and aluminum alloys make them promising candidates for automotive light-weighting but standard phenomenological plasticity models cannot adequately capture the complex plastic response of these materials. In this study, the constitutive plastic behavior of a rare-earth magnesium alloy sheet, ZEK100 (O-temper), was considered at room temperature, under quasi-static conditions. The CPB06 yield criterion for hcp materials was employed along with a non-associative flow rule in which the yield function and plastic potential were calibrated for a range of plastic deformation levels to account for evolving anisotropy under proportional loading. The non-associative flow rule has not previously been applied to magnesium alloys which require the use of flexible constitutive models to capture the severe anisotropy and its evolution with plastic deformation. The non-associative flow rule can provide the required flexibility by decoupling the yield function and plastic potential. For the associative flow rule, such flexibility can only be achieved by multiple linear transformations of the stress tensor resulting in expensive models for calibration and simulations. The constitutive model was implemented as a user material subroutine (UMAT) within the commercial finite element software, LS-DYNA, for general 3-D stress states along with an interpolation technique to consider the evolution of anisotropy based upon the plastic work. To evaluate the accuracy of the implemented model, predictions of a single-element model were compared with the experimental results in terms of flow stresses and plastic flow directions under various proportional loading conditions and along different test directions. Finally, to assess the predictive capabilities of the model, full-scale simulations of coupon-level formability experiments were performed and compared with experimental results in terms of far-field load-displacement and local strain paths. Using these experiments, the constitutive model was evaluated across the full range of representative stress states for sheet metal forming operations. It was shown that the predictions of the model were in very good agreement with experimental data.
The objective of the current study is to develop a practical, deterministic approach to the prediction of the in-plane formability of two third generation advanced high-strength steels (AHSS) of 980 and 1180 MPa ultimate tensile strength using only quasi-static mechanical property data. The hardening response to large strains was experimentally measured with the use of simple shear and tensile tests and validated in tensile simulations. The process-corrected limit strains in the Nakazima and Marciniak tests were compared to various analytical Forming Limit Curve (FLC) models for in-plane stretching. It was observed that the widely-used Marciniak–Kuczynski model can adequately predict the experimental FLC in biaxial stretching but significantly underestimated the limit strains in uniaxial stretching for both third generation AHSS. The observed through-thickness shear fracture mode in biaxial stretching was reasonably well-captured by the Bressan–Williams (BW) instability model for the 1180 MPa steel. A proposed extension of the BW model to uniaxial tension by adoption of the maximum in-plane shear stress criterion (BWx model) provided superior experimental correlation relative to the zero-extension model of Hill that was too conservative. Finally, a linearized version of the modified maximum force criterion (MMFC) was proposed that markedly improved the correlation with the process-corrected FLC for in-plane stretching of AHSS. The developed framework for FLC prediction was then applied to a DP980 AHSS and an AA5182 aluminum alloy from the literature. The DP980 corroborated the observed trend for the two third generation AHSS whereas the MK and the BWx models performed best for the AA5182 with its saturation-type hardening behavior and non-quadratic yield surface.
The present study investigates how the choice of characterization test and the composition of the stress state in terms of tension and shear can produce a non-unique failure locus in terms of stress triaxiality under plane stress conditions. Stress states that are composed of tensile and simple shear loadings result in a loss of proportionality between the cumulative strain and stress such that the principal frames become non-coaxial despite a constant stress triaxiality. Consequently, it is shown that the conventional interpretation of a failure locus in plane stress is based upon an implicit assumption of proportional coaxial loading. The use of simple shear tests along with traditional in-plane tensile tests for fracture characterization is only one “path” that can be taken in terms of the stress triaxiality, which may produce a bifurcation at uniaxial tension while the tension–torsion path does not. In general, the failure locus in terms of the equivalent strain is a failure surface and must consider the composition of the stress state that produces a given triaxiality. A comprehensive review of phenomenological fracture loci within a modified Mohr-Coulomb (MMC) framework is performed to highlight how the choice of stress states obtained using different characterization tests can change the apparent fracture locus of a material. The finite strain solutions for the work conjugate equivalent strain are derived for various loading paths that produce the same stress triaxiality. It is then shown that accounting for non-coaxiality leads to equivalent failure strains that are even higher than previously reported in tension–torsion tests within the literature. The equivalent plastic strains integrated from finite-element simulations are work-conjugate by definition. The equivalent strains estimated from the cumulative principal strains using DIC strain measurement depend upon a coaxial or non-coaxial assumption. Finally, an analytical solution for the onset of diffuse necking that accounts for the stabilizing influence of shear loading against a tensile instability is considered. Even under plane stress conditions, a failure surface arises in terms of the equivalent strain at necking, the stress triaxiality, and the severity of shear loading.