Friction stir welding (FSW) is an alternative method to join aluminum (Al) alloys in a solid-state condition. However, the coarsening or dissolution of precipitation hardening phases in the welding zone causes strength reduction or softening behavior in the welded area of age-hardened Al alloys. Therefore, this research aimed to improve the mechanical properties of an FSW Al–Mg–Si alloy via post-weld heat treatment (PWHT) and the possibility of controlling the abnormal grain growth (AGG) using different welding parameters. FSW was performed with different rotational and travel speeds, and T6 heat treatment was carried out on the FSW samples as the PWHT. The results showed a decrease in the strength of the FSW samples compared with that of the base material (BM) due to the dissolution of precipitation hardening particles in the heat-affected zone. However, the emergence of AGG in the microstructure after the T6-PWHT was identified as the potential event in the microstructure of the PWHT samples. It is found that the AGG of the microstructure in similar joints of Al6061(T6) was governed by the welding parameters. The results proved that PWHT was able to increase the tensile properties of the welded samples to values comparable to that of Al6061(T6)-BM. The increased mechanical properties of the FSW joints were attributed to a proper PWHT that resulted in a homogeneous distribution of the precipitation hardening phases in the welding zones.
1 September 2013 in International Journal of Automotive and Mechanical Engineering
Aluminium alloys are lightweight materials relatively used in automotive industries. However, welding using the conventional welding methods is known to be difficult. In this study, the friction stir welding (FSW) known as the solid state joining process was extensively used for joining similar and dissimilar 5 mm aluminium alloy plates. The butt-joint type of similar joints (AA5083-AA5083) and dissimilar joints (AA5083- AA6061) were carried out under the same welding parameters; 1000 rpm (rotational speed) and 100 mm/min (transverse speed). Macro- and microstructural observations were acquired at the cross-section of the weld regions by stereo and optical microscopes. The microstructural study showed that the formation of ‘onion ring’ structure was detected in the nugget zone of similar joints, while wavy and distorted patterns appeared in dissimilar joints. All tensile specimens of similar welding joint showed similar fracture patterns where all fractures occurred in the thermo-mechanically affected zone (TMAZ). However, tensile specimens of dissimilar welding joint broke up at the TMAZ region as well as at Al6061 base metal at the retreating side. The tensile strength of similar joint and dissimilar joint was 22% and 19% lower compared to the base metal of Al5083 and Al6061.