Vapor phase transport (VPT) assisted by mixture of methanol and acetone via thermal evaporation of brass (CuZn) was used to prepare un-doped and Al-doped zinc oxide (ZnO) nanostructures (NSs). The structure and morphology were characterized by field emission scanning electron microscopy (FESEM) and x-ray diffraction (XRD). Photoluminescence (PL) properties of un-doped and Al-doped ZnO showed significant changes in the optical properties providing evidence for several types of defects such as zinc interstitials (Zni), oxygen interstitials (Oi), zinc vacancy (Vzn), singly charged zinc vacancy (VZn-), oxygen vacancy (Vo), singly charged oxygen vacancy (Vo+) and oxygen anti-site defects (OZn) in the grown NSs. The Al-doped ZnO NSs have exhibited shifted PL peaks at near band edge (NBE) and red luminescence compared to the un-doped ZnO. The Raman scattering results provided evidence of Al doping into the ZnO NSs due to peak shift from 145 cm-1 to an anomalous peak at 138 cm-1. Presence of enhanced Raman signal at around 274 and 743 cm-1 further confirmed Al in ZnO NSs. The enhanced D and G band in all Al-doped ZnO NSs shows possible functionalization and doping process in ZnO NSs.
Zinc oxide (ZnO) nanowires (NWs) were synthesized using vapor phase transport (VPT) and thermal evaporation of Zn from CuZn. Time dependence of ZnO NWs growth was investigated for 5, 10, 15, 20, 25, and 30 minutes. Significant changes were observed from the field electron scanning electron microscopy (FESEM) images as well as from the X‐ray diffraction (XRD) profile. The photoluminescence (PL) profile was attributed to the contribution of oxygen vacancy, zinc interstitials, and hydrogen defects in the ZnO NWs. Raman scattering results show a significant peak at 143 cm−1 and possible functionalization on the wall of ZnO NWs. Growth of ZnO NWs in (0002) with an estimated distance between adjacent lattice planes 0.26 nm was determined from transmission electron microscopy (TEM) analysis.
10 November 2017 in Optical and Quantum Electronics
The drop casting method is utilized on indium tin oxide (ITO)-coated glass in order to prepare a sandwiched ITO/graphene oxide (ITO/GO) with silicon dioxide/p-type silicon (SiO2/p-Si) heterojunction photodetector. The partially sandwiched GO layer with SiO2/p-Si substrate exhibits dual characteristics as it showed good sensitivity towards the illumination of infrared (IR) laser at wavelength of 974 nm. Excellent photoconduction is also observed for current–voltage (I–V) characteristics at various laser powers. An external quantum efficiency greater than 1 for a direct current bias voltage of 0 and 3 V reveals significant photoresponsivity of the photodetector at various laser frequency modulation at 1, 5 and 9 Hz. The rise times are found to be 75, 72 and 70 μs for 1, 5 and 9 Hz while high fall times 455, 448 and 426 are measured for the respective frequency modulation. The fabricated ITO/GO-SiO2/p-Si sandwiched heterojunction photodetector can be considered as a good candidate for applications in the IR regions that do not require a high-speed response.