Radiation-related caries is a unique form of rampant decay and is a complication of head and neck radiotherapy that frequently causes generalized dental destruction and impairs quality of life in cancer patients. The aim of this study was to investigate the patterns of demineralization of caries in irradiated patients and to establish whether direct radiogenic damage to the dentition might be important in the progression of radiation-related caries. Teeth from patients who had concluded radiotherapy were examined histologically by polarized light microscopy, and the ultrastructure was examined by scanning backscattered electron microscopy. Cervical caries and incisal caries, a very unusual sort of lesion, were widely detected. Additionally, diffuse brown discoloration of the smooth surface of enamel was frequently observed. Polarized light microscopy suggested that these areas were incipient caries. Evidence of normal odontoblast function was observed in the detection of reactionary dentin and intratubular dentin deposition. In conclusion, radiation-related caries seems to have the same morphological and demineralization pattern as ordinary caries, with the presence of demineralized dentin, a translucent zone, dentin dead tracts, reactionary dentin and intratubular dentin deposition. Based on these findings, direct radiogenic destruction of the teeth seems to be not essential to the microscopic progression of radiation-related caries.
1 January 2013 in International Journal of Dentistry
Purpose.This study investigated the long-term resin-dentin bond strength of dentin biomodified by proanthocyanidin-rich (PA) agents.Materials and Methods.Forty molars had their coronal dentin exposed, etched, and treated for 10 minutes with 6.5% grape seed extract (GSE), 6.5% cocoa seed extract ethanol-water (CSE-ET), 6.5% cocoa seed extract acetone-water (CSE-AC), and distilled water (CO). Samples were restored either with One-Step Plus (OS) or Adper Single-Bond Plus (SB). Bond strength test was performed immediately or after 3, 6, and 12 months.Results.HigherμTBS were observed for GSE immediately (SB- 62.9 MPa; OS- 51.9 MPa) when compared to CSE-ET (SB- 56.95 MPa; OS- 60.28 MPa), CSE-AC (SB- 49.97 MPa; OS- 54.44 MPa), and CO (SB- 52.0 MPa; OS- 44.0 MPa) (). CSE outcomes were adhesive system and solvent dependant. After 12 months storage SB results showed no difference among treatment types (GSE- 57.15 MPa; CSE/ET- 54.04 MPa; CSE/AC- 48.22 MPa; CO- 51.68 MPa;),while OS results where treatment dependent (GSE- 42.62 MPa; CSE/ET- 44.06 MPa; CSE/AC- 41.30 MPa; CO- 36.85 MPa;).Conclusions.GSE and CSE-ET agents provided enhanced immediate adhesion and stabilization to demineralized dentin after long-term storage, depending on adhesive system.
The purpose of this study was to evaluate the effect of replacing a component of the self-etch adhesive Adper Scotchbond SE (liquid A + liquid B) by 2% chlorhexidine (CHX) on bond strength to dentin after 1 day, 3 months or 6 months of water storage. Eight human teeth were sectioned to expose a flat dentin surface and were then randomly assigned to 2 groups. In the control group, the dentin surfaces were treated with the adhesive according to the manufacturer's instructions. In the experimental group, liquid A was replaced by 2% CHX. Next, a 6-mm-high resin composite block was incrementally built on the bonded surfaces. The restored teeth were then sectioned to produce stick-shaped specimens (cross-sectional area - 0.8 mm2). The microtensile bond strength (µTBS) was recorded, and the failure modes were assessed. Data were analyzed by two-way repeated measures ANOVA (α=0.05). Four additional teeth were processed in order to conduct a micromorphological analysis of the resin-dentin interface. The µTBS values did not significantly decrease after water storage in either the control or the experimental group, whose values did not differ significantly irrespective of storage time. The morphological aspect of the bonding interface appears not to have been affected by CHX. A higher incidence of cohesive failures within the adhesive and mixed failures (cohesive within adhesive and resin composite) was observed for both groups. It may be concluded that dentin pre-treatment with 2% CHX did not influence significantly the bonding performance of the evaluated adhesive.
1 January 2021 in Restorative Dentistry & Endodontics