Hanqin Liang

Dr. Hanqin Liang


Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
22 April 2021 in RSC Advances
Verified
Journal Article
Open access
PDF file
YMYu Ma
Yu Ma
HLHanqin Liang
Hanqin Liang
JYJinwei Yin
Jinwei Yin
DYDongxu Yao
Dongxu Yao
YXYongfeng Xia
Yongfeng Xia
YZYuping Zeng
Yuping Zeng
Charcoal monoliths derived from waste wood were activated with air for the application of electrochemical capacitor electrodes and an insight was given into the activation mechanism. The mild air activation is effective and pollution-free compared to the common chemical activation using KOH etc. for the preparation of crack-free carbon monoliths. The activation process was controlled by altering the activation temperature and time, and their effects on the nanostructure of charcoal monoliths were studied. As the activation temperature or time increased, air eroded the defective surface of charcoal layer-by-layer, with the oxygen atoms being introduced by chemisorption and oxidation reactions and removed by dehydration and decomposition reactions. Meanwhile, micro-pores were produced. The electrode activated at 300 °C for 1 h, with a specific surface area of 567 m2 g−1 and a high micro-porosity of 86%, exhibited a specific capacitance of 203 F g−1 and 35.5 F cm−3. Moreover, it presented a higher total capacitance of 3.6 F cm−2 than most reported pellet electrodes. These findings give a reasonable picture of the air activation process and are instructive to prepare activated carbon monoliths under an oxidizing environment.

1 January 2016 in Journal of Inorganic Materials
Verified
Journal Article
Closed access
HLHanqin Liang
Hanqin Liang
YXYao Xiu-Min
Yao Xiu-Min
ZHZhengren Huang
Zhengren Huang
ZYZeng Yu-Ping
Zeng Yu-Ping
The densification process of liquid phase sintered SiC ceramics with Al 2 O 3 and Y 2 O 3 as sintering additives was investigated by in situ measurement apparatus combined with conventional methods. The shrinkage curve, morphology of the sample and liquid phase formation process simulation were observed by high temperature in-situ observation furnace. The relative density, flexural strength and microstructure evolution were characterized by analysis of samples sintered at temperatures ranging from 1640℃ to 1920℃ at 40℃ interval. The obvious temperature that liquid phase began to function was confirmed between 1640℃ to 1680℃. The classical liquid phase sintering theory was testified. Highly-densified SiC ceramics were obtained by being sintered at 1880℃, of which the relative density was (99.46 ± 0.37)%, and the flexural strength was (650 ± 26) MPa.

1 January 2021 in Journal of Inorganic Materials
Verified
Journal Article
Closed access
PDF file
HLHanqin Liang
Hanqin Liang
JYJinwei Yin
Jinwei Yin
KZKaihui Zuo
Kaihui Zuo
YXYongfeng Xia
Yongfeng Xia
DYDongxu Yao
Dongxu Yao
YZYuping Zeng
Yuping Zeng