Structural, optical and electrical properties of (ytterbium/terbium) co-doped ZnO thin films deposited on glass substrates using the spray pyrolysis method were investigated. The films exhibited the hexagonal wurtzite structure with a preferential orientation along (002) direction. No secondary phase was observed in the X-ray diffraction detection limit. Atomic force microscopy (AFM) was performed and root means square roughness (RMS) of our samples decreased with terbium content. Photoluminescence measurements showed a luminescence band at 980 nm which is characteristic of Yb3+ transition between the electronic levels 2F5/2 to 2F7/2. This is experimental evidence for an efficient energy transfer from the ZnO matrix to Yb. Hall Effect measurements gave a low electrical resistivity value around 6.0 × 10−3 Ω.cm. Such characteristics make these films of interest to photovoltaic devices.
In doped ZnO (IZO), In-Al co-doped ZnO (IAZO) and In-F co-doped ZnO (IFZO) were deposited on glass substrates at 350 °C by spray pyrolysis technique. The structural, optical and electrical properties of as-deposited thin films were investigated and compared. A polycrystalline and (002) oriented wurtzite crystal structure was confirmed by X-ray patterns for all films; and the full width at half-maximum (FWHM) of (002) diffraction peak increased after co-doping. The investigation of the optical properties was performed using Uv-vis spectroscopy. The average transmittances of all the films were between 70 and 85%. Hall Effect measurements showed that the electrical conductivity of co-doped films increased as compared with IZO thin film. The highest conductivity of about 16.39 Ω-1 cm-1 was obtained for as-deposited IFZO thin film. In addition, the thin films were annealed at 350 °C for two hour under Ar atmosphere and their optical, electrical properties and the associated photoluminescence (PL) responses of selected films were analysed. After annealing, the electrical conductivity of all thin films was improved and the optical transmittance remained above 70%. Room temperature PL revealed that the annealed IAZO thin film had a strong green emission than that of IZO film.
Undoped ZnO, Gd doped ZnO (GZO) thin films were prepared by chemical spray pyrolysis method at 350°C on glass substrates. The effect of gadolinium doping on structural, morphological, optical and electrical properties as function of dopant concentration has been studied. X-ray analysis showed that the films are polycrystalline fitting well with hexagonal wurtzite structure and have preferred orientation in [002] direction. The AFM analysis showed that the grain size as well as the roughness of the Gd doped ZnO films constantly decreases with increasing dopant content. The deposited films showed an average optical transmittance around 85% in the visible region and the optical band gap of the ZnO:Gd films decreases from 3.27 eV to 3.18 eV as dopant content increases. Hall Effect measurements showed that electrical conductivity, mobility carriers and carrier concentration of the films are increased after 1.5 % Gd doping concentration.
YbxEryZnO thin films with a low concentration (x = 5%, y = 0, 1, 3%) were made on glass substrates using the spray pyrolysis method. The films were characterized through the use of specific techniques to investigate their structural, optical, and electrical properties. The XRD structural analysis of the films revealed that they are polycrystalline with a hexagonal wurtzite structure and a preferential orientation in the (002) direction. The optical characterization of the co-doped layers in the range of 200 to 800 nm revealed that co-doping had a significant impact on the values of transmission. A well-defined peak in the infrared domain centered around 980 nm was observed in photoluminescence measurements. This peak signifies the transition between the electronic levels 2F5/2 (ground state) and 2F7/2 (excited state), proving that photons are efficiently transferred between the ZnO matrix and the Yb3+ ion. All layers exhibited n-type conduction and an electrical resistivity decrease to 6.0 × 10−2 Ω cm according to Hall effect measurements at room temperature.