Cunshan Wang

Prof. Dr. Cunshan Wang


Research Focus & Metrics

Academic Career Length

20Years (2007-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
28 September 2007 in Journal of Materials Science
Verified
Journal Article
Closed access
PDF file
CWCunshan Wang
Cunshan Wang
KZK. S. Zhang
K. S. Zhang
HPH. J. Pang
H. J. Pang
YCY. Z. Chen
Y. Z. Chen
CDC. Dong
C. Dong

7 October 2017 in Metals
Verified
Journal Article
Open access
PDF file
LZLuan Zhang
Luan Zhang
CWCunshan Wang
Cunshan Wang
SQShengnan Qian
Shengnan Qian
QYQun Yu
Qun Yu
Chuang DongChuang Dong
Chuang Dong
It has been reported that a quaternary Co61.2B26.2Si7.8Ta4.8 alloy is a good glass former and can be laser-clad to an amorphous composite coating with superior hardness and wear resistance. In this paper, alloys with varying Ni contents to substitute for Co are coated on the surface of #45 carbon steel using a 5-kW CO2 laser source for the purpose of obtaining protective coatings. In contrast to the quaternary case, the clad layers are characterized by a matrix of α-(Fe, Co, Ni) solid solution plus CoB, Co3B, and Co3Ta types of precipitates. The cladding layer is divided into four regions: Near-surface dendrites, α-(Fe, Co, Ni) solid solution plus dispersed particles in the middle zone, columnar bonding zone, and heat-affected area that consists of martensite. The hardness gradually decreases with increasing Ni content, and the maximum hardness occurs in the middle zone. Both the friction coefficient and wear volume are minimized in the alloy containing 12.2% Ni. Compared with the previous cobalt-based quaternary alloy Co61.2B26.2Si7.8Ta4.8, the addition of the Ni element reduces the glass-forming ability and henceforth the hardness and wear resistance of the clad layers.

25 January 2023 in Materials
Verified
Journal Article
Open access
PDF file
JZJingtao Zhang
Jingtao Zhang
CWCunshan Wang
Cunshan Wang
NSNisha Shareef
Nisha Shareef
The binary Ti-Zr congruent alloys have been a potential candidate for laser-directed energy deposition owing to an excellent combination of high structural stability and good formability. To solve its insufficient strength, a new series of Ti-Zr-Mo alloys with different Mo contents were designed based on a cluster model and then made by laser-directed energy deposition on a high-purity titanium substrate. The effect of Mo content on the microstructure and properties of the L-DEDed alloys was investigated. The consequences exhibit that the microstructure of all designed alloys is featured with near-equiaxed β grains without obvious texture. However, increasing Mo content induces a gradual refinement of the grain and a steady decrease in the lattice constant, which effectively improves the hardness, strength, wear and corrosion resistance of the designed alloys, but slightly weakens ductility and formability. From the viewpoint of both properties and forming quality, the Ti60.94Zr36.72Mo2.34 (at.%) alloy owns a proper match in mechanical, tribological, chemical, and forming properties, which is widely used in aeroengine components.

3 May 2022 in RSC Advances
Verified
Journal Article
Open access
PDF file
XZXue Zhang
Xue Zhang
CWCunshan Wang
Cunshan Wang
WYWenfei Yang
Wenfei Yang
DGDongdong Gao
Dongdong Gao
ZZZhongyuan Zhang
Zhongyuan Zhang
XDXinglong Dong
Xinglong Dong
Integrated Al/Ni electrodes of lithium-ion batteries (LIBs) with variant atomic ratios were successfully fabricated by a one-step laser-sintering process. The microstructure, phase composition, and pore structure were controlled by the raw material composition and laser parameters. The electrodes showed working merits without any conductive agent and binder, or even the collector used in a traditional battery. It was shown that the electrode consisted of multi-phases, i.e., Al, Al3Ni2, Al3Ni, and Ni, when the Al/Ni atomic ratio was higher than 5 : 5. A lower Al/Ni atomic ratio less than 5 : 5 favored the formation of a dual-phase electrode consisting of Al3Ni2 and Ni. As the Al content increased, the specific surface area of the as-sintered electrodes increased in the initial stage and then decreased. The formation of pores was closely related to the content of the residual Al phase after the laser sintering. The residual Al phase filled the pores when the Al content was high, leading to a lower pore size. In contrast, the liquid Al phase completely reacted with the Ni component, leaving a large number of pores at its original sites. The linked pores can serve as transport channels for Li+ ions, provide mass sites for electrochemical reactions, and also buffer huge volume changes of the active material. Among the electrodes, the one with an Al/Ni ratio of 3 : 7 showed the best cycling/rate performance, i.e., a capacity of 522.8 mA h g−1 by a current of 0.1 A g−1 after 200 cycles, even holding to 338.4 mA h g−1 by a big current impact at 2 A g−1. It formed a metallurgical combination between the conductive network and the active material with multiple porous structures, which is helpful for the electrodes to provide high capacity and maintain structural stability during cycling. In addition, the average laser-sintering time of a single electrode was within 10 s, which is suitable for industrial mass production.