Top-contact bottom-gate thin film transistors (TFTs) with zinc-rich indium zinc tin oxide (IZTO) active layer were prepared at room temperature by radio frequency magnetron sputtering. Sintered ceramic target was prepared and used for deposition from oxide powder mixture having the molar ratio of In2O3:ZnO:SnO2 = 2:5:1. Annealing treatment was carried out for as-deposited films at various temperatures to investigate its effect on TFT performances. It was found that annealing treatment at 350 °C for 30 min in air atmosphere yielded the best result, with the high field effect mobility value of 34 cm2/Vs and the minimum subthreshold swing value of 0.12 V/dec. All IZTO thin films were amorphous, even after annealing treatment of up to 350 °C.
ZnO thin film field effect transistors with 1.5–20μm gate width were fabricated using either a metal gate [metal–semiconductor field effect transistor (MESFET)] or a metal–oxide–semiconductor (MOS) gate. In both cases we found that use of a thick (∼0.8–0.9μm) ZnO buffer was necessary on the sapphire or glass substrate prior to growing the active layers in order to reduce gate leakage current. Source/drain contacts of e-beam deposited Ti∕Al∕Pt∕Au showed specific contact resistances of 2.18×10−6Ωcm2 without annealing and the interdevice isolation currents were ∼10μA at 40V bias. The MOS structure with 50nm (Ce,Tb)MgAl11O19 gate dielectric showed a 1 order of magnitude lower gate leakage current than the MESFET, due to the relatively low barrier height of metals on n-type ZnO (0.6–0.8eV). Good drain–source current characteristics were obtained from MOS gate structures using P-doped ZnO channels, whereas the metal structures showed very poor modulation.
This study reports on the fabrication of quantum dot light‐emitting diodes (QLEDs) with an ITO/Ni
1−
x Mg x O/SAM/TFB/QDs/ZnMgO/Al structure and investigates the effects of various Mg doping concentrations in NiO on device performance. By doping Mg into the inorganic hole‐injection layer NiO (Ni
1−
x Mg x O), we improved the band alignment with the hole‐injection layer through band tuning, which enhanced charge balance. Optimal Mg doping ratios, particularly a Ni 0.9 Mg 0.1 O composition, have demonstrated superior device functionality, underscoring the need for fine‐tuned doping levels. Further enhancements were achieved through surface treatments of Ni 0.9 Mg 0.1 O with UV‐Ozone (UVO) and thermal annealing (TA) of the ZnMgO electron transport layer. Consequently, by optimizing Mg‐doped NiO in QLED devices, we achieved a maximum external quantum efficiency of 8.38 %, a brightness of 66,677 cd/m 2 , and a current efficiency of 35.31 cd/A, indicating improved performance. The integration of Mg‐doped NiO into the QLED structure resulted in a device with superior charge balance and overall performance, which is a promising direction for future QLED display technologies.