This paper demonstrates a simple method to fabricate 3D microchannels and microvasculature at room temperature by direct-writing liquid metal as a sacrificial template. The formation of a surface oxide skin on the low-viscosity liquid metal stabilizes the shape of the printed metal for planar and out-of-plane structures. The printed structures can be embedded in a variety of soft (e.g. elastomeric) and rigid (e.g. thermoset) polymers. Both acid and electrochemical reduction are capable of removing the oxide skin that forms on the metal, which destabilizes the ink so that it withdraws from the encapsulating material due to capillary forces, resulting in nearly full recovery of the fugitive ink at room temperature. Whereas conventional fabrication procedures typically confine microchannels to 2D planes, the geometry of the printed microchannels can be varied from a simple 2D network to complex 3D architectures without using lithography. The method produces robust monolithic structures without the need for any bonding or assembling techniques that often limit the materials of construction of conventional microchannels. Removing select portions of the metal leaves behind 3D metal features that can be used as antennas, interconnects, or electrodes for interfacing with lab-on-a-chip devices. This paper describes the capabilities and limitations of this simple process.
Traditional hollow metallic waveguide manufacturing techniques are readily capable of producing components with high-precision geometric tolerances, yet generally lack the ability to customize individual parts on demand or to deliver finished components with low lead times. This paper proposes a Rapid-Prototyping (RP) method for relatively low-loss millimeter-wave hollow waveguides produced using consumer-grade stere-olithographic (SLA) Additive Manufacturing (AM) technology, in conjunction with an electroless metallization process optimized for acrylate-based photopolymer substrates. To demonstrate the capabilities of this particular AM process, waveguide prototypes are fabricated for the W- and D-bands. The measured insertion loss at W-band is between 0.12 dB/in to 0.25 dB/in, corresponding to a mean value of 0.16 dB/in. To our knowledge, this is the lowest insertion loss figure presented to date, when compared to other W-Band AM waveguide designs reported in the literature. Printed D-band waveguide prototypes exhibit a transducer loss of 0.26 dB/in to 1.01 dB/in, with a corresponding mean value of 0.65 dB/in, which is similar performance to a commercial metal waveguide.