The purpose of this paper is to investigate the mechanisms of cracking and failure in fiber metal laminates (FMLs) subjected to 3-point bending. Two types of laminates, based on the glass/epoxy and carbon/epoxy composites, were selected for the study. The paper presents the failures of matrix and fibers as well as the effects of different thicknesses of metal layers on the tested laminates. The mechanisms of failure observed for the two tested types of fibers with uniform thickness of aluminum sheets seem similar. The results demonstrate that the tested laminates exhibit the following failure modes: fiber breakage, matrix cracking, fiber/matrix debonding, delamination, and anodic layer failure. Given the behavior of aluminum under the compressive and tensile stresses, the aluminum layer acts as a barrier preventing FML failure during bending. In addition to aluminum layer thickness, the fiber type and composite layer directions are also important factors to be considered.
Fiber metal laminates (FMLs) are the hybrid laminates consisting of alternating thin layers of metal sheets and fiber-reinforced composite material. Interface between metal and polymer layer plays a significant role. FMLs have both low density and high relative strength, and other good properties as high damage tolerance: fatigue and impact characteristics, corrosion, and fire resistance. In present work, the microstructure of the aluminum-epoxy/glass and aluminum-epoxy/carbon composites is characterized. The interface between metal and polymer composites with surface treatment and without surface treatment at different pressures was examined. It was observed that pretreatment of the aluminum has a significant effect on the zone between metal and polymer composite. In the interface, there is a direct contact between anodizing layer and resin without fibers, the same for epoxy/glass and epoxy/carbon laminates. The low pressure in autoclave process has a detrimental effect on the structure. It is responsible for the formation of the porosity and delamination in polymer layer and interface between aluminum and polymer composites. Untreated surface of aluminum sheet is characterized by too low adhesion to epoxy composite, especially with carbon reinforcement.
1 July 2014 in Aircraft Engineering and Aerospace Technology
Fiber metal laminates (FMLs) were initially developed under the motivation of the aerospace industry. Generally, they consist of aluminum and high strength glass fiber in polymeric layers, but the new challenge is to apply them with a carbon fiber. Pretreatment of aluminum is the main factor responsible for the adhesion between metallic and polymeric layers. The shear strength test a very popular method in the experimental joint of two components. In this article, the main aim was to compare the surface pretreatment and configuration of fibers in FMLs based on aluminum with glass and carbon fibers. The decisive factor of strength in adhesive or cohesive failure is first the type of fibers, and second, the surface preparation.
The aim of the study was to assess the selected properties of a hybrid organic–inorganic silane sol–gel coating (HSG) used in hybrid fiber metal laminates (FML) in a corrosion environment. The HSG coating on the aluminum alloy was produced using 3M™ AC130-2 formulation consisting of 3-glycidoxypropyl-trimethoxysilane (GPTMS) and tetra-n-propoxyzirconium (zirconium(IV) propoxide) (TPOZ). Laminates consisted of aluminum alloy AA2024-T3 sheets, with carbon fiber reinforced polymers (CFRPs) and a glass fiber reinforced metal–composite structure (GFRP). Potentiodynamic and polarization curve and impedance (EIS) tests were carried out on HSG at ambient temperatures after 1 h and 150 h of soaking. Neutral 0.5 M NaCl and 0.8 M NaCl solutions were used for open circuit potential (OCP) and potentiodynamic tests, and 0.5 NaCl was used for the EIS test. A neutral salt spray (NSS) test was applied to laminates with a 12 week exposure period. The results obtained revealed that the HSG coating did not provide sufficient protection against corrosion of the aluminum alloy in direct contact with an aggressive environment but was effective as an interlayer. Local aluminum sheet perforation did not lead to delamination at the metal–composite interface regardless of the type or configuration of the composite. This confirms the durability of HSG used in FMLs.
17 November 2020 in Journal of Asian Ceramic Societies
In recent years, magnesium alloys have become a subject of interest in many industrial sectors, e.g. the automotive and aircraft industries as well as biomedical and mechanical engineering. Magnesium alloys belong to the group of the lightest alloys of non-ferrous metals. Therefore, their application in the aircraft industry is a very desirable solution. The innovative combination of a composite layer with carbon fibers in aviation on the same principle as fiber metal laminates encourages thorough analysis of the corrosive behavior of the connection of two chemically different materials. As is known, such a connection is greatly exposed to corrosion, especially galvanic, between its components. Therefore, the corrosion behavior of the magnesium alloy with a protective coating must first be examined before joining with the CFRP layer. The present article is the first one in a series of analyses carried out in order to evaluate the corrosion resistance and behavior of the AZ31 alloy with plasma electrolytic oxidation (PEO) and a primer in an NaCl solution. Those results show that among Mg/PEO, Mg/Primer and Mg/PEO/Primer has the best corrosion resistance due to Mg/PEO/Primer possess the PEO and primer layer simultaneously.