We report a novel approach in fabricating high-performance enhancement mode (E-mode) AlGaN/GaN HEMTs. The fabrication technique is based on fluoride-based plasma treatment of the gate region in AlGaN/GaN HEMTs and post-gate rapid thermal annealing with an annealing temperature lower than 500/spl deg/C. Starting with a conventional depletion-mode HEMT sample, we found that fluoride-based plasma treatment can effectively shift the threshold voltage from -4.0 to 0.9 V. Most importantly, a zero transconductance (g/sub m/) was obtained at V/sub gs/=0 V, demonstrating for the first time true E-mode operation in an AlGaN/GaN HEMT. At V/sub gs/=0 V, the off-state drain leakage current is 28 μA/mm at a drain-source bias of 6 V. The fabricated E-mode AlGaN/GaN HEMTs with 1 μm-long gate exhibit a maximum drain current density of 310 mA/mm, a peak g/sub m/ of 148 mS/mm, a current gain cutoff frequency f T of 10.1 GHz and a maximum oscillation frequency f max of 34.3 GHz.
21 August 2006 in IEEE Transactions on Electron Devices
This paper presents a method with an accurate control of threshold voltages (Vth) of AlGaN/GaN high-electron mobility transistors (HEMTs) using a fluoride-based plasma treatment. Using this method, the Vth of AlGaN/GaN HEMTs can be continuously shifted from -4 V in a conventional depletion-mode (D-mode) AlGaN/GaN HEMT to 0.9 V in an enhancement-mode AlGaN/GaN HEMT. It was found that the plasma-induced damages result in a mobility degradation of two-dimensional electron gas. The damages can be repaired and the mobility can be recovered by a post-gate annealing step at 400 degC. At the same time, the shift in Vth shows a good thermal stability and is not affected by the post-gate annealing. The enhancement-mode HEMTs show a performance (transconductance, cutoff frequencies) comparable to the D-mode HEMTs. Experimental results confirm that the threshold-voltage shift originates from the incorporation of F ions in the AlGaN barrier. In addition, the fluoride-based plasma treatment was also found to be effective in lowering the gate-leakage current, in both forward and reverse bias regions. A physical model of the threshold voltage is proposed to explain the effects of the fluoride-based plasma treatment on AlGaN/GaN HEMTs
We report an AlGaN/GaN/InGaN/GaN double heterojunction high electron mobility transistors (DH-HEMTs) with high-mobility two-dimensional electron gas (2-DEG) and reduced buffer leakage. The device features a 3-nm thin In/sub x/Ga/sub 1-x/N(x=0.1) layer inserted into the conventional AlGaN/GaN HEMT structure. Assisted by the InGaN layers polarization field that is opposite to that in the AlGaN layer, an additional potential barrier is introduced between the 2-DEG channel and buffer, leading to enhanced carrier confinement and improved buffer isolation. For a sample grown on sapphire substrate with MOCVD-grown GaN buffer, a 2-DEG mobility of around 1300 cm 2 /V/spl middot/s and a sheet resistance of 420 /spl Omega//sq were obtained on this new DH-HEMT structure at room temperature. A peak transconductance of 230 mS/mm, a peak current gain cutoff frequency (f T ) of 14.5 GHz, and a peak power gain cutoff frequency (f max ) of 45.4 GHz were achieved on a 1×100 μm device. The off-state source-drain leakage current is as low as /spl sim/5 μ A/mm at V/sub DS/=10 V. For the devices on sapphire substrate, maximum power density of 3.4 W/mm and PAE of 41% were obtained at 2 GHz.
26 December 2006 in IEEE Transactions on Electron Devices
We present the detailed dc and radio-frequency characteristics of an Al0.3Ga0.7N/GaN/In0.1Ga0.9 N/GaN double-heterojunction HEMT (DH-HEMT) structure. This structure incorporates a thin (3 nm) In0.1Ga0.9N notch layer inserted at a location that is 6-nm away from the AlGaN/GaN heterointerface. The In0.1Ga0.9N layer provides a unique piezoelectric polarization field which results in a higher potential barrier at the backside of the two-dimensional electron gas channel, effectively improving the carrier confinement and then reducing the buffer leakage. Both depletion-mode (D-mode) and enhancement-mode (E-mode) devices were fabricated on this new structure. Compared with the baseline AlGaN/GaN HEMTs, the DH-HEMT shows lower drain leakage current. The gate leakage current is also found to be reduced, owing to an improved surface morphology in InGaN-incorporated epitaxial structures. DC and small- and large-signal microwave characteristics, together with the linearity performances, have been investigated. The channel transit delay time analysis also revealed that there was a minor channel in the InGaN layer in which the electrons exhibited a mobility slightly lower than the GaN channel. The E-mode DH-HEMTs were also fabricated using our recently developed CF4-based plasma treatment technique. The large-signal operation of the E-mode GaN-based HEMTs was reported for the first time. At 2 GHz, a 1times100 mum E-mode device demonstrated a maximum output power of 3.12 W/mm and a power-added efficiency of 49% with single-polarity biases (a gate bias of +0.5 V and a drain bias of 35 V). An output third-order interception point of 34.7 dBm was obtained in the E-mode HEMTs
We report an Al/sub 0.3/Ga/sub 0.7/N-Al/sub 0.05/Ga/sub 0.95/N-GaN composite-channel HEMT with enhanced linearity. By engineering the channel region, i.e., inserting a 6-nm-thick AlGaN layer with 5% Al composition in the channel region, a composite-channel HEMT was demonstrated. Transconductance and cutoff frequencies of a 1 ×100 μm HEMT are kept near their peak values throughout the low- and high-current operating levels, a desirable feature for linear power amplifiers. The composite-channel HEMT exhibits a peak transconductance of 150 mS/mm, a peak current gain cutoff frequency (f T ) of 12 GHz and a peak power gain cutoff frequency (f max ) of 30 GHz. For devices grown on sapphire substrate, maximum power density of 3.38 W/mm, power-added efficiency of 45% are obtained at 2 GHz. The output third-order intercept point (OIP3) is 33.2 dBm from two-tone measurement at 2 GHz.