This paper addresses the study of the complex effect of alloying elements (magnesium, manganese, copper and zirconium) on changes in magnesium-rich aluminum alloy composition, fine and coarse particle size and number, recrystallization characteristics and mechanical properties. The data obtained made it possible to analyze change in the chemical composition, sizes of intermetallic compounds and dispersoids depending on alloying elements content. The effect of the chemical composition on the driving force and the number of recrystallization nuclei was studied. It was established that the addition of alloying elements leads to grain refinement, including through the activation of a particle-stimulated nucleation mechanism. As a result, with Mg increase from 4 to 5%, addition of 0.5% Mn and 0.5% Cu, the grain size decreased from 72 to 15 µm. Grain refinement occurred due to an increase in the number of particle-stimulated nuclei, the number of which at minimal alloying rose from 3.47 × 1011 to 81.2 × 1011 with the maximum concentration of Mg, Mn, Cu additives. The retarding force of recrystallization, which in the original alloy was 1.57 × 10−3 N/m2, increased to 5.49 × 10−3 N/m2 at maximum alloying. The influence of copper was especially noticeable, the introduction of 0.5% increasing the retarding force of recrystallization by 2.39 × 10−3 N/m2. This is due to the fact that copper has the most significant effect on the size and number of intermetallic particles. It was established that strength increase without ductility change occurs when magnesium, manganese and copper content increases.
Bimetallic materials are important in many industries (aerospace, medicine, etc.) since they allow the creation of constructions that combine specific functional properties, for example, low density (aluminum alloy) and high corrosion resistance (stainless steel), due to layering fabrication of the bimetallic joint. On the other hand, the difference in thermophysical properties of the dissimilar material layers leads to residual stresses, which cause deformation and destruction of such a bimetallic joint produced via the methods of surfacing or additive technologies. This article discusses the methods based on the gray relational analysis and generalized desirability function for the quality assessment of Al–10Si–Mg aluminum alloy and Cr18–Ni10–Ti stainless-steel bimetal fabricated via selective laser melting (SLM). There are four main parameters (quality indices) of the quality generalized assessment, which determine the degree of Al penetration into the steel substrate and Fe into the deposited layer, the difference in microhardness values on both sides of the interface boundary, and the resistance to mechanical destruction of the bimetallic joint. According to the results obtained, the best set of quality indices corresponds to the SLM technological modes with an energy density of 105 and 147 J/mm3. The greatest functionality of the bimetals is determined by the quality index associated with its strength. Therefore, methods of gray relational analysis and desirability function make it possible to form a generalized assessment for the bimetallic joint quality and, consequently, to select the best technological mode.
25 May 2016 in STRUCTURAL ENGINEERING AND MECHANICS
The freeform capability additive manufacturing (AM) technique and the magnetic efficiency of Fe-6.5Si steel have the potential for the development of electromechanical component designs with thin body sections. Moreover, the directional anisotropy of the material, which is formed during growth, improves the magnetic and electrical properties of Fe-6.5 wt%Si. We obtained the range of optimal technological modes of Laser Power Bed Fusion process (volume energy density (VED) of 100–140 J/mm3, scanning speed of 750–500 mm/s) to produce the samples from Fe-6.5 wt%Si powder, but even at the best of them cracks may appear. The optical microscopy and SEM with EDX analysis of the laser-fabricated structures are applied for investigation of this phenomena. We detected a carbon content at the boundaries of the cracks. This suggests that one of the reasons for the crack formation is the presence of Fe3C in the area of the ordered phases. Quantitative analysis based on crack initiation criteria (CIC) showed that the safe level of internal stresses in terms of the CIC criteria in the area of discontinuities is exceeded by almost 190%. Local precipitates of carbides in the area of cracks are explained by the heterogeneity and high dynamics of temperature fields, as well as the transfer of substances due to Marangoni convection, which, as a result, contributes to a significant segregation of elements and the formation of precipitate phases.
1 January 2016 in Advances in Materials Science and Engineering
This paper examines the effect of the yield criterion of the matrix on brittle fracture of the fibre in continuous fibre reinforced metal matrix composites subjected to tension in the direction parallel to the fibres. It is assumed that the matrix obeys quite a general isotropic yield criterion. An approximate approach to predicting the tensile load at which the fibre breaks previously proposed in the literature is adopted. It is shown that this tensile load is practically independent of the yield criterion of the matrix. This is a great advantage for engineering applications since an analytic solution is available in the case of Tresca yield criterion. This solution can be used for a wide range of matrix materials with no loss of the accuracy of the prediction of the tensile load at which the fibre breaks.
1 January 2015 in Russian Journal of Non-Ferrous Metals
Theoretical notions and formation modes of the crystallographic texture of sheets made of the V95pch aluminum alloy, which intensifies the formation of parts made of glass-fiber reinforced aluminum laminates by stretch forming, are presented. The deformation texture (orientations S and Bs) is formed during hot rolling; it becomes stronger during further cold rolling. The recrystallization texture is formed during annealing (orientations [011]〈100〉, [023]〈100〉). An increase in the limiting stretch-forming coefficient after cold rolling is provided by two-stage annealing, which includes rapid heating at the continuous heat treatment line and subsequent complete annealing in an in-and-out furnace with slow cooling.