This research aimed to investigate the effects of bismuth (Bi) and phosphorus (P) addition on the microstructure and roughness of a B390 hypereutectic Al-Si alloy. Microstructural variation of as-cast alloys showed that P is an effective refiner of primary Si and its distribution, while Bi has the opposite effect. The liquidus temperature increased with greater amounts of P, resulting in a wider solidification range. The solidus temperature increased with Bi content, resulting in a shortened solidification range. The benefit of Bi on eutectic silicon was through changing its morphology from fibrous to lamellar structures. It was observed that both primary Si and eutectic Si were modified when both P and Bi were added to the alloys. For effective refinement, the size of primary Si can be reduced by 50.6% and, the P content should not be less than 0.1 wt% with a Bi content of 0.5–1.0 wt%. Furthermore, an intermetallic phase size reduction also occurs. P addition results in a significant (5.85%) increase in hardness. Adding Bi (up to 1.0 wt%) together with P (up to 0.1 wt%) did not reduce the effect of P on the hardness of the modified alloys. The most effective reduction in roughness achieved during cutting at both low and high speeds was 26.5% and 57.7%, respectively, from modifying the B390 alloy using 0.1 wt%P with 1.0 wt%Bi.
This research focuses on the fabrication of Al7075 composites reinforced with varying amounts of nano-sized SiC particles (1.0, 1.5, and 2.0 wt%) combined with 0.5 wt% graphite (Gr), employing a hybrid process of mechanical alloying and semi-solid stir casting. The study investigates the influence of SiC content, nanoparticle feeding method, and the role of Gr on the microstructures, mechanical characteristics, and machinability of the composites. Microstructural analysis revealed that integrating milled powders into the molten Al7075 alloy produced a uniform dispersion of nanoscale SiC particles within the α-Al matrix, avoiding the particle agglomeration observed with the conventional method. Higher SiC content resulted in finer grains and improved mechanical performance. The Al7075-0.5Gr-2.0SiC composite exhibited a 16% increase in hardness relative to the unreinforced Al7075 alloy. The inclusion of nanoscale SiC particles notably enhanced tensile strength, while the presence of Gr acted as a lubricant, improving surface roughness.
This research investigated the rheo-die-casting process and the production of an A356/silicon carbide (SiC) composite by a thixoforming. The composite contained 15 percent by weight SiC particles of around 15–37 µm in size as the reinforcing phase. The composite feedstock was produced by semi-solid stir-casting, where pretreated SiC powder was gradually added into the A356 alloy melt to form a continuously stirred slurry composite melt, which was then cast in a steel mold. For thixoforming, the feedstock was reheated to 583 °C (approximately 0.4 fraction liquid), and its viscosity was reduced with shear rate, implying that A356/SiC exhibits shear thinning or non-Newtonian behavior. This is caused by the characteristic billet structure obtained having relatively globular grains that accommodate the flow of the semisolid composite. In the rheo-die-casting process, the A356/SiC feedstock was re-melted at 610–615 °C (approximately 0.8–0.9 fraction liquid) prior to die-casting and the resulting slurry was injected into a die with injection speeds of 3 and 4 m/s and pressures of 11 and 12 MPa, respectively. Two work-pieces of 16 × 15.6 × 205 mm3 were produced in one shot, and the resulting samples were subjected to T6 solution treatment at 540 °C for 1 h, quenched, and aged at 135 °C for 12 h. The results show that both low speed and low pressure rheo-die-cast samples exhibit uneven filling at the end of the part, whilst both high pressure and high speed promote more uniform distribution of SiC particles throughout the part length. In the as-rheo-die-cast condition, the most uniform of microstructures and hardness obtained from a sample fabricated at 4 m/s speed and 12 MPa pressure.
This study aims to investigate patient waiting time in General Practice Clinic and identify the main cause of the problem through patient satisfaction survey. 9,232 Patients were randomly observed and quantitative data such as arrival time and waiting time were recorded. Other 1,200 patients were randomly selected for satisfaction survey which is considered as qualitative data. The result indicated that average waiting time of patients was 175.87 minutes with standard deviation of 68.66 minutes. Waiting time at GP clinic appeared to be the longest with an average of 92.9 minutes and standard deviation of 43.4 minutes. Also, based on the obtained data, patients remained positive until their waiting time exceeded 2 hours.