Yonghui Lin

Dr. Yonghui Lin

Hebei Normal University for Nationalities
orcid

Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 April 2020 in Materials
Verified
Journal Article
Open access
PDF file
Yonghui LinYonghui Lin
Yonghui Lin
DXDongqiang Xu
Dongqiang Xu
XZXianhui Zhao
Xianhui Zhao
Soda residue (SR), the solid waste of Na2CO3 produced by ammonia soda process, pollutes water and soil, increasing environmental pressure. SR has high alkalinity, and its main components are Ca(OH)2, NaCl, CaCl2, CaSO4, and CaCO3, which accords with the requirements of being an alkali activator. The aim of this research is to investigate the best proportion of SR addition and the contribution of individual chemical components in SR to SR- activated ground granulated blast furnace slag (GGBS) cementitious materials. In this paper, GGBS pastes activated by SR, Ca(OH)2, Ca(OH)2 + NaCl, Ca(OH)2 + CaCl2, Ca(OH)2 + CaSO4, and Ca(OH)2 + CaCO3 were studied regarding setting time, compressive strength (1 d, 3 d, 7 d, 14 d, 28 d), hydration products, and microstructure. The results demonstrate that SR (24%)-activated GGBS pastes possess acceptable setting time and compressive strength (29.6 MPa, 28 d), and its hydration products are calcium silicate hydrate (CSH) gel, calcium aluminum silicate hydrates (CASH) gel and Friedel’s salt. CaCl2 in SR plays a main role in hydration products generation and high compressive strength of SR- activated GGBS pastes.

27 May 2021 in Materials
Verified
Journal Article
Open access
PDF file
Yonghui LinYonghui Lin
Yonghui Lin
DXDongqiang Xu
Dongqiang Xu
XZXianhui Zhao
Xianhui Zhao
Soda residue (SR), an industrial solid waste, pollutes the environment due to its high alkalinity and chloride ion content. SR can be used as an alkali activator of ground granulated blast furnace slag (GGBFS). This study investigated the effects of four types of SR-activated GGBFS cementitious materials (pastes) with different mass ratios of SR to GGBFS (8:92, 16:84, 24:76, 34:68) on the physical properties, mechanical strength, and chloride binding capacity. The hydration mechanism of the pastes was also studied. Results showed that with the increasing addition of SR, the density of the pastes decreased, and more white aggregates of SR appeared causing the increase of water absorption and porosity of the pastes. The pastes with 16% SR addition had the maximum compressive strength (34.1 MPa, 28 d), so the optimum proportion of SR addition in the pastes was 16%. With the increases of SR addition, the amount of chloride element in the initial pastes increases. When the proportion of SR addition is 8%, the mass percentage of free chloride ion in the pastes at 28 d is 0.13%. The main hydration products of the pastes were C–S–H gels, ettringite, and Friedel’s salt, and the amount of ettringite varied with the amount of SR addition and curing time.

7 February 2021 in Materials
Verified
Journal Article
Open access
PDF file
XZXianhui Zhao
Xianhui Zhao
HWHaoyu Wang
Haoyu Wang
Boyu ZhouBoyu Zhou
Boyu Zhou
Han GaoHan Gao
Han Gao
Yonghui LinYonghui Lin
Yonghui Lin
The early mechanical performances of low-calcium fly ash (FFA)-based geopolymer (FFA–GEO) mortar can be enhanced by soda residue (SR). However, the resistance of SR–FFA–GEO mortar to acid or sulfate environments is unclear, owing to the various inorganic calcium salts in SR. The aim of this study was to investigate the long-term mechanical strengths of up to 360 d and evaluate the resistance of SR–FFA–GEO mortar to 5% HCl and 5% Na2SO4 environments through the losses in compressive strength and mass. Scanning Electron Microscopy (SEM), Energy-Dispersive Spectroscopy (EDS) and Fourier Transform Infrared Spectrometer (FTIR) experiments were conducted for the SR–FFA–GEO mortars, both before and after chemical attack, to clarify the attack mechanism. The results show that the resistances of the SR–FFA–GEO mortar with 20% SR (namely M10) to 5% HCl and 5% Na2SO4 environments are superior to those of cement mortar. The environmental HCl reacts with the calcites in SR to produce CaCl2, CO2 and H2O to form more pores under HCl attack, and the environmental Na+ cations from Na2SO4 go into Si-O-Al network structure, to further enhance the strength of mortar under Na2SO4 attack. These results provide the experimental basis for the durability optimization of SR–FFA–GEO mortars.

8 December 2020 in Materials
Verified
Journal Article
Open access
PDF file
Haoyu WangHaoyu Wang
Haoyu Wang
XZXianhui Zhao
Xianhui Zhao
Boyu ZhouBoyu Zhou
Boyu Zhou
Yonghui LinYonghui Lin
Yonghui Lin
HGHan Gao
Han Gao
Solid waste soda residue (SR), as an industrial pollutant of water, air and soil environment, can be utilized to prepare the low-calcium fly ash (FFA)-based geopolymer paste activated by sodium silicate (NS) solution for goaf backfill. However, the high addition of NS produces the high cost and high strength of synthesized backfill material in the previous study. The objective of this research is to investigate the cost optimization method and performance evaluation of SR-FFA-based geopolymer backfill paste. The alkaline beta-hemihydrate gypsum (BHG) alternative to partial NS was proposed. Scanning electron microscopy (SEM), X-ray diffraction (XRD) as well as Fourier transform infrared spectrometer (FTIR) tests were performed to clarify the role of BHG and evaluate the microstructures and products of backfill pastes. The results show that 10% BHG alternative ratios effectively improve fluidity, setting time and compressive strength to satisfy the performance requirement of goaf backfill material. The gel products in the optimal backfill paste C4 with 10% BHG alternative ratios are determined as the coexistence of C-S-H gel, (N,C)-A-S-H gel and CaSO4·2H2O at 28 d. The research results can make extensive utilization of SR and FFA in cemented paste backfill to synthesize cleaner material at a larger scale.

15 February 2022 in Advances in Materials Science and Engineering
Verified
Journal Article
Open access
PDF file
HWHaoyu Wang
Haoyu Wang
XZXianhui Zhao
Xianhui Zhao
TWTing Wang
Ting Wang
LSLei Su
Lei Su
Boyu ZhouBoyu Zhou
Boyu Zhou
Yonghui LinYonghui Lin
Yonghui Lin
The introduction of soluble calcium additives contributes to forming calcium-containing geopolymer (N,C)-A-S-H and/or calcium (alumino)silicate hydration C-(A)-S-H in alkali-activated fly ash-based composites (AAFCs). However, the quantitative determination of the final gel product has yet been unclear due to the different chemical components, which influences the prediction of mechanical strength and microstructure. This study aims to propose a method to clarify the gel products in AAFCs by the critical elemental compositions in gel products. Furthermore, the AAFCs were prepared (by casting method) using soda residue (SR) as the calcium additive, fly ash as the aluminosilicate precursor, and sodium silicate solution as the alkaline activator. The compressive strengths of the AAFCs with different SR contents were recorded. The microstructures and gel products of AAFCs were detected through scanning electron microscope (SEM), energy-dispersive spectroscopy (EDS), X-ray diffraction (XRD), and 29Si nuclear magnetic resonance spectrometer (29Si NMR). Finally, the proposed determination method was verified with the experimental results. The new proposed quantitative method refers to a limit value of 2Ca/Al=1.00 about the critical chemical elements in gel products, which helps to determine the calcium-containing geopolymer (N,C)-A-S-H or/and calcium (alumino)silicate hydration C-(A)-S-H in stable AAFCs. Results show that the gel products are determined as single (N,C)-A-S-H gels when 2Ca/Al is lower than 1.00; meanwhile, (N,C)-A-S-H and C-(A)-S-H gels coexist when 2Ca/Al is higher than 1.00 by the above proposed quantitative determination method. Furthermore, it works that the industrial solid waste SRs regarded as calcium additive are applied in the AAFCs to verify the gel products by 2Ca/Al=1.00 as the limit value. The results provide the theoretical and experimental basis for the performance prediction and microstructural determination.

17 May 2022 in Materials
Verified
Journal Article
Open access
PDF file
Yonghui LinYonghui Lin
Yonghui Lin
DXDongqiang Xu
Dongqiang Xu
WJWenguang Ji
Wenguang Ji
XZXianhui Zhao
Xianhui Zhao
Soda residue (SR), a solid waste generated in the production of Na2CO3 during the ammonia soda process, with a high pH value of 12, can be used as an activator of alkali-activated ground granulated blast furnace slag (GGBFS) cementitious materials. Three groups of experiments on SR-activated GGBFS mortars were designed in this paper to assess the role of the dominant parameters on fluidity and compressive strength of mortars. The results indicate that for fluidity and mechanical properties, the optimal scheme of SR-activated GGBFS mortars is 16:84–24:76 S/G, 0.01 NaOH/b, 0.05 CaO/b, and 0.50 w/b, with fluidity and compressive strength (28 d) of the mortars being 181–195 mm and 32.3–35.4 MPa, respectively. Between 2.5–10% CaCl2 addition to CaO (5%)-SR (24%)-activated GGBFS mortar is beneficial to the improvement of the compressive strength of C2, whereas the addition of CaSO4 is harmful. The main hydration products of mortars are ettringite, Friedel’s slat, and CSH gels. The results provide a theoretical basis and data support for the utilization of SR.