High surface area activated carbon fibers (ACF) have been prepared from bamboo by steam activation after liquefaction and curing. The influences of activation temperature on the microstructure, surface area and porosity were investigated. The results showed that ACF from bamboo at 850 °C have the maximum iodine and methylene blue adsorption values. Aside from the graphitic carbon, phenolic and carbonyl groups were the predominant functions on the surface of activated carbon fiber from bamboo. The prepared ACF from bamboo were found to be mainly type I of isotherm, but the mesoporosity presented an increasing trend after 700 °C. The surface area and micropore volume of samples, which were determined by application of the Brunauer-Emmett-Teller (BET) and t-plot methods, were as high as 2024 m2/g and 0.569 cm3/g, respectively. It was also found that the higher activation temperature produced the more ordered microcrystalline structure of ACF from bamboo.
In order to improve the outdoor exposure performance of laminated bamboo, boric acid/borax and UV absorbents, including triazole (UV1130), nano–TiO2, and nano–SiO2, were used to modify waterborne polyurethane (WPU) coatings, respectively. The physical and chemical properties of the coatings with and without modification were evaluated by adhesion strength, contact angle, wear, and temperature-resistance experiments. The antimildew properties of the coatings were evaluated by the bacteriostatic zone method, and the pyrolysis characteristics were investigated through TG–FTIR analysis. The results showed that, when compared with the unmodified WPU coating, the coatings with different modifications had stronger wear resistance; the mass loss of the best C4 coating was only 0.0078 g, which was 0.0203 g less than that of the unmodified C0 coating. However, when compared to the unmodified coating, the wettability of the modified coating increased to different degrees, and the contact angle of the C4 coating with the most obvious effect was only 36.50°. During the curing process of the modified coatings, the UV absorbents and boric acid/borax would interact with the C–N, C–O, and C=O bonds in the coating and change the molecular structure of the WPU. The thermal stability of the coatings with different modifications was enhanced. The best result, a 76.27% weight loss, was observed in the modified coating with boric acid/borax and 1.0% nano–TiO2. Different modified coatings had a certain degree of control effect on Aspergillus Niger, and the reason for this was considered the combined effect of boric acid/borax and UV absorbents.
The effects of different UV absorbents and preservatives on the weatherability of modified waterborne polyurethane (WPU) printed laminated bamboo were investigated. Three types of UV absorbents including 2-hydroxy-4-n-octoxy-benzophenone (UV-531), 2-(2 H-benzotriazol-2-yl)-4-(1,1,3,3 tetramethylbutyl) phenol (UV-329), and nano-TiO2, and four types of preservatives including boric acid (BA), borax (BX), ammonium polyphosphate (APP), and disodium octaborate tetrahydrate (DOT) were selected to modify WPU coatings. The printed laminated bamboo was tested to evaluate the coating physical and chemical properties and dimensional stability. Thirteen coating types were tested. The results showed that the 0 (20% WPU), 5 (UV-531-BA/BX), 6 (UV-531-BA/BX/APP), 7 (UV-531-BA/BX/DOT), 8 (UV-531-BA/BX/APP/DOT), and 9 (nano-TiO2/BA/BX) samples performed well in adhesion, abrasion resistance, hardness, and temperature denaturation. Fourier transform infrared (FT-IR) spectra analyses and dimensional stability analysis were carried out on the six kinds of coatings screened out. FT-IR spectra analyses showed the successful introduction of UV light absorbers and flame retardants, whereas test results of hygroscopicity showed that the coated test material improved the dimensional stability performance. Test material 8(UV-531-BA/BX/APP/DOT) had the best dimensional stability performance.
Southern pine (Pinus sp.) wood cubes were treated with ACQ solutions with wax modification and post-treated at 70 °C for 10 h with hot air circulation. The effects of wax concentrations in ACQ-treated southern pine on its dimensional stability and copper leaching performance were investigated. The ACQ/wax-treated wood exhibited improved water resistance during the water soak process. The testing of swelling and shrinkage performance of the treated wood showed that samples with a higher percentage of wax had higher resistance to water swelling and shrinkage. The samples with a lower percentage of wax addition had only a slight effect on the moisture swelling and shrinkage resistance. As a result, copper leaching from ACQ/wax-treated wood with a 2% wax concentration was reduced to a lower level compared to ACQ-treated wood. When the proportion of wax in ACQ preservative was less than 1%, a higher percentage of copper was leached from treated wood.
Southern yellow pine (Pinus sp.) wood cubes were vacuum-pressure treated with nano-SiO2 solution and different concentrations of amine copper quaternary (ACQ)/wax (0.5%, 2.5%, and 5.0% wax)-modified solutions. The effects of wax concentration and nano-SiO2 addition on water absorption, air drying shrinkage, and moisture swelling stabilities were investigated. The results showed that during the whole process of water absorption and air drying shrinkage, better stability of nano-SiO2 modified ACQ-treated wood could only be obtained with the ratio of wax addition equal to 2.5%. However, the best moisture swelling resistance was found in the samples modified with the highest wax addition (5.0%). Both wax and nano-SiO2 could be useful for keeping the dimensional stability of the treated wood.