Ciprofloxacin (CIP), as a representative broad-spectrum antibiotic, poses a major threat to human health and the ecological environment as a result of its abuse and emissions. In this study, a highly active Mn2+-oxidizing bacterium, Pseudomonas sp. CCTCC M2014168, was induced to form micro-/nanostructured biogenic Mn oxide (BMO) aggregates through continuous culturing with 1 mmoL−1 Mn2+. Following the characterization of Mn4+ oxides and the micro-/nanostructures by scanning electron microscopy, high-resolution transmission electron microscopy and X-ray diffraction assays, the BMO composites were subjected to CIP degradation and detoxification in laboratory trials. High-performance liquid chromatograph (HPLC) analysis identified that the BMO composites were capable of completely degrading CIP, and HPLC with a mass spectrometer (LC/MS) assays identified three intermediates in the degradation pathway. The reaction temperature, pH and initial ciprofloxacin concentration substantially affected the degradation efficiency of CIP to a certain extent, and the metal ions Mg2+, Cu2+, Ni2+ and Co2+ exerted significant inhibitory effects on CIP degradation. A toxicity test of the degradation products showed that CIP was completely detoxified by degradation. Moreover, the prepared BMO composite exhibited a high capacity for repeated degradation and good performance in continuous degradation cycles, as well as a high capacity to degrade CIP in real natural water.
A biotemplated cation-incoporating method based on bacterial cell-surface display technology and biogenic Mn oxide mineralization process was developed to fabricate Mn-based multiphasic composites as anodes for Li-ion batteries. The engineered Pseudomonas putida MB285 cells with surface-immobilized multicopper oxidase serve as nucleation centers in the Mn oxide biomineralization process, and the Mn oxides act as a settler for incorporating Ni ions to form aggregates in this process. The assays using X-ray photoelectron spectroscopy, phase compositions, and fine structures verified that the resulting material MnO/C/NiO (CMB-Ni) was porous multiphasic composites with spherical and porous nanostructures. The electrochemical properties of materials were improved in the presence of NiO. The reversible discharge capacity of CMB-Ni remained at 352.92 mAh g−1 after 200 cycles at 0.1 A g−1 current density. In particular, the coulombic efficiency was approximately 100% after the second cycle for CMB-Ni.
Manganese oxidizing bacteria can produce biogenic manganese oxides (BMO) on their cell surface and have been applied in the fields of agriculture, bioremediation, and drinking water treatment to remove toxic contaminants based on their remarkable chemical reactivity. Herein, we report for the first time the synthetic application of the manganese oxidizing bacteria, Pseudomonas putida MnB1 as a whole-cell biocatalyst for the effective oxidation of β-keto ester with excellent yield. Differing from known chemical protocols toward this transformation that generally necessitate the use of organic solvents, stoichiometric oxygenating agents and complex chemical catalysts, our strategy can accomplish it simply under aqueous and mild conditions with higher efficiency than that provided by chemical manganese oxides. Moreover, the live MnB1 bacteria are capable of continuous catalysis for this C-O bond forming reaction for several cycles and remain proliferating, highlighting the favorable merits of this novel protocol for sustainable chemistry and green synthesis.
Manganese oxides reportedly exhibit pronounced adsorption capacities for numerous heavy-metal ions owing to their unique structural properties. Herein, a biogenic manganese oxide (BMO) composite was developed and used to remove Ni ions from Ni2+-containing electroplating wastewater. The formation of BMO and the micro-/nanoscale fine microstructure were characterized via scanning/high-resolution transmission electron microscopies and X-ray diffraction assays. Under the optimized conditions, with an adsorption temperature of 50 °C, pH 6, the BMO composite showed a 100% removal efficiency within a rapid equilibrium reaction time of 20 min towards an initial Ni2+ concentration of 10 mg L−1 and a remarkable removal capacity of 416.2 mg g−1 towards an initial Ni2+ concentration of 600 mg L−1 in Ni-electroplating wastewater. The pseudo-second-order equation was applicable to sorption data at low initial Ni2+ concentrations of 10–50 mg L−1 over the time course. Moreover, Freundlich isotherm models fitted the biosorption equilibrium data well. Fourier-transform infrared spectroscopic analysis validated that the removal capacity of the BMO composite was closely associated with structural groups. In five continuous cycles of adsorption/desorption, the BMO composite exhibited high Ni2+ removal and recovery capacities, thereby showing an efficient and continuous performance potential in treating Ni2+-containing industrial wastewater.