In recent years, researchers have explored the interlayer stacking structure of the bilayer (BL) transition metal dichalcogenides (TMDCs) and found that it has unique impact on the electrical, optical, and vibrational properties of TMDCs. Unfortunately, the size of BL TMDCs synthesized by the pre-existing methods is not large. In addition, there is not any effective mean to control the number of layers as well as the stack structure. This is the major limiting factor for further exploration of the properties of BL TMDCs. We report a new method for the rapid and controllable growth of AB-stacked BL MoS 2 . Firstly, the mixed solution of Na 2 MoO 4 and NaOH was spun on the sapphire substrate and then sulfurated. The BL MoS 2 of AB-stacked can be obtained by changing the time of sulfur introduction. The size of the BL MoS 2 is related to the parameters of sulfur. The maximum size of BL MoS 2 grown by this method can reach 288 μ m, and the average size can reach about 200 μ m, which is larger than the size reported in most articles. In addition, the growth rate of BL MoS 2 can be clearly increased by the spin-coating growth method and the fastest growth rate is up to 144 μ m min −1 , which is far higher than other published reports at present. Subsequently, a photodetector based on BL MoS 2 was prepared. The response time of rising edge is about 0.32 ms, and that of falling edge is about 3.2 ms. The detector prepared by us shows excellent photoelectric detection performance. Therefore, the excellent performance of BL MoS 2 makes it have a broad application prospect in the field of high-performance electronics and optoelectronics.
Bioresorbable electronic devices and/or systems are of great appeal in the field of biomedical engineering due to their unique characteristics that can be dissolved and resorbed after a predefined period, thus eliminating the costs and risks associated with the secondary surgery for retrieval. Among them, passive electronic components or systems are attractive for the clear structure design, simple fabrication process, and ease of data extraction. This work reviews the recent progress on bioresorbable passive electronic devices and systems, with an emphasis on their applications in biomedical engineering. Materials strategies, device architectures, integration approaches, and applications of bioresorbable passive devices are discussed. Furthermore, this work also overviews wireless passive systems fabricated with the combination of various passive components for vital sign monitoring, drug delivering, and nerve regeneration. Finally, we conclude with some perspectives on future fundamental studies, application opportunities, and remaining challenges of bioresorbable passive electronics.
The metal/germanium (Ge) photodetectors have attracted much attention for their potential applications in on-chip optoelectronics. One critical issue is the relatively large dark current due to the limited Schottky potential barrier height of the metal/germanium junction, which is mainly caused by the small bandgap of Ge and the Fermi energy level pinning effect between the metal and Ge. The main technique to solve this problem is to insert a thin interlayer between the metal and Ge. However, so far, the dark current of the photodetectors is still large when using a bulk-material insertion layer, while when using a two-dimensional insertion layer, the area of the insertion layer is too small to support a mass production. Here, we report a gold/graphene/germanium photodetector with a wafer-scale graphene insertion layer using a 4 inch graphene-on-germanium wafer. The insertion layer significantly increases the potential barrier height, leading to a dark current as low as 1.6 mA cm−2, and a responsivity of 1.82 A W−1 which are the best results for metal/Ge photodetectors reported so far. Our work contributes to the mass production of high-performance metal/Ge photodetectors.
In this study, the growth kinetics of SiGe in a reduced pressure chemical vapor deposition system using dichlorosilane (SiH2Cl2) and germane (GeH4) as the Si and Ge precursors were investigated. The SiGe growth rate and Ge content were found to depend on the deposition temperature, GeH4 flow and reactor chamber pressure. The SiGe growth rate escalates with increasing deposition temperature, while the Ge content is reduced. The SiGe growth rate accelerates with increasing GeH4 flow, while the Ge content increases more slowly. According to the experimental data, a new relationship between Ge content (x) and F(GeH4)/F(SiH2Cl2) mass flow ratio is deduced: x2.5/(1−x) = nF(GeH4)/F(SiH2Cl2). The SiGe growth rate and Ge content improve with increasing reactor chamber pressure. By selecting proper precursor flows and reactor pressure, SiGe films with the same Ge content can be fabricated at various temperatures. However, the quality of the SiGe crystals is clearly dependent on the deposition temperature. At lower deposition temperature, higher crystalline quality is achieved. Because the growth rate dramatically drops with lower temperatures, the optimum growth temperature must be a compromise between the crystalline quality and the growth rate. X-ray diffraction, Raman scattering spectroscopy and atomic force microscopy results indicate that 650°C is the optimum temperature for fabrication of Si0.75Ge0.25 film.