Ductile iron is a high-strength cast iron material. The spherical graphite obtained by inoculation treatment effectively improves the mechanical properties of cast iron, resulting in higher strength than carbon steel. However, severe corrosion may occur under specific circumstances, especially in thermal water pipelines. In this paper, the corrosion mechanisms at the main defective points of ductile iron were investigated using microscopic morphological characterization after accelerated tests combined with numerical simulations. The influence law of each environmental factor on the corrosion kinetics of ductile iron in a complex water quality environment was studied using dynamic potential polarization tests. The results showed that the main causative factors leading to the increased corrosion of ductile iron were the presence of tail-like gaps on its surface, and the crescent-shaped shrinkage and loosening organization around the graphite spheres. After mechanical treatment was applied to eliminate the obvious defects, the number of corrosion pits was reduced by 41.6%, and the depth of the pits was slowed down by 40% after five days. By comparison, after ten days, the number of pits was reduced by 51%, and the depth of the pits was slowed down by 50%. The dynamic potential polarization test results show that the dissolved oxygen concentration has the greatest influence on the corrosion of ductile iron in the simulated water environment; meanwhile, the water hardness can slow down the corrosion of ductile iron. The relative influence of each environmental factor is as follows: dissolved oxygen concentration > temperature > immersion time > water hardness > pH > Cl−.
This study investigates the impact of Ca and Sb elements on the corrosion resistance of E690 steel in a simulated marine environment. Electrochemical testing and dry/wet cyclic corrosion testing were conducted on prepared E690 steel specimens. The eroded specimens’ microstructure was observed under a scanning electron microscope, and the inclusion morphology was analyzed using an energy-dispersive spectrometer (EDS). The simulating liquid was designed to emulate the severe marine atmospheric environment in Xisha. Results showed that the addition of Ca and Sb elements effectively enhances the corrosion resistance of E690 steel in the simulated marine environment. The corrosion rates of E690 steel specimens with Ca and Sb additions were lower than those without, and the corrosion morphology was more uniform. These findings suggest that the addition of Ca and Sb elements can improve the corrosion resistance of E690 steel in simulated marine environments and have potential for use in marine engineering applications.
The structural design of steel–titanium composite plates significantly affects their corrosion resistance. To investigate the impact of defects of different shapes and sizes on the corrosion behavior of steel–titanium composite plates, this study designed six types of defects and conducted a series of characterization tests. The results showed that due to the galvanic interaction between carbon steel and titanium alloy, small defects initially accelerate corrosion, resulting in 50% to 200% more corrosion weight loss compared to large defects. However, in the later stages of immersion, the corrosion rate of small defects decreased by up to 35%, which was attributed to the accumulation of protective corrosion products. Additionally, there is an inverse relationship between the corrosion rate and the thickness ratio of the composite plate. The reduction in the area of Q345B also results in additional corrosion loss of up to 32%.
Based on actual service environment parameters, this experiment investigated the change in the corrosion rate of nodular cast iron (DCI) in an environment containing organic (triethanolamine phosphate, PTEA) and inorganic (hexametaphosphate, SHMP) inhibitors, and analyzed the effects of both inhibitors and the pH value of the solution on the corrosion behavior of DCI. Additionally, a variable flow rate device was used to conduct immersion tests, enabling the accurate evaluation of the materials’ corrosion resistance in an actual service environment. After a certain period, the corrosion of the DCI surface was observed, and the weight loss corrosion rate of the materials was calculated to analyze the differences in corrosion resistance under varying environmental parameters. It was found that the inhibitory effect of both inhibitors on DCI increased with the immersion time, and the inhibitory effect of the SHMP inhibitor was more pronounced under alkaline conditions. Based on the electrochemical and flow rate immersion test results, it can be concluded that, in the solution environment used in this experiment, the inhibitory effect of the SHMP inhibitor on DCI is stronger than that of the PTEA inhibitor.