Globally, thermal power plants produce about 780 million tonnes of coal ash, of which Asia alone accounts for 66% of this share. India, the third-largest coal ash producer, generated 226 million metric tonnes in 2019. Conserving natural resources and promoting viable alternatives are priorities that contribute to achieving sustainable development goals. This study aims to assess the fresh and hardened properties of high-strength concrete, in which 75% of natural fine aggregate (NFA) is supplemented with coal bottom ash (CBA). This study assessed ultrasonic pulse velocity and compressive strength at 3, 7, 28, 56, and 90 days using 100 mm cube specimens, split tensile and flexural strength at 7 and 28 days with 150 mm dia. × 300 mm height cylindrical specimens and 500×100×100 mm beam specimens, respectively. A minimum of three samples are tested in each group per test, and the average values are recorded. The findings reveal promising outcomes for using high-volume CBA as a feasible alternative to NFA. The concrete exhibited commendable early-age hardened properties with a 28-day compressive strength of 79.73 MPa, flexural strength of 7.2 MPa, and split tensile strength of 3.25 MPa, supporting the suitability of CBA in high-strength applications. The higher water absorption of CBA due to its porous structure may have led to a higher slump value. However, it's important to note that a higher slump value meant that the slump was a collapse pattern, and the mix also showed significant bleeding, segregation, and a longer setting time, which presents a considerable challenge when attempting to incorporate higher volumes of CBA into concrete.
The search for viable alternative resources is essential for advancing sustainable development in the construction industry. A significant global concern is the substantial generation of industrial waste, particularly coal ash byproducts such as fly ash (FA) and coal bottom ash (CBA) from thermal power plants (TPPs). India ranks as the third-largest producer of coal ash globally and the second-largest in Asia, generating approximately 105 million metric tonnes annually. While TPP-derived wastes have been extensively studied in masonry mortars, the potential of CBA as a partial or complete replacement for natural fine aggregates (NFA) in high-strength mortar (HSM) remains significantly underexplored. This study investigates the fresh, mechanical, and microstructural properties of mortar incorporating CBA as a substitute for NFA, specifically up to a 100% replacement level Flow table tests revealed improved workability with increasing CBA content, which is attributed to its porous microstructure; however, significant bleeding was observed at higher replacement levels (≥75%). The dry density consistently decreased with the addition of CBA with a reduction of up to 19.27% at full replacement. Ultrasonic pulse velocity (UPV) values declined with higher levels of CBA but improved with curing age. The mortar incorporating up to 100% CBA retains appreciable mechanical properties despite a progressive reduction in compressive strength (CS) with increasing CBA content. The observed compressive strengths for the different mixes were as follows: control mix (CM) at 36.72 MPa, mix with 25% CBA (CBA25) at 25.56 MPa, mix with 50% CBA (CBA50) at 19.69 MPa, mix with 75% CBA (CBA75) at 16 MPa, and mix with 100% CBA (CBA100) at 9.93 MPa. All mixes exceeded the minimum strength criteria, confirming their classification as HSMs at all replacement levels. These results highlight the potential of CBA as a sustainable alternative in construction materials, supporting efforts toward resource efficiency and environmental sustainability in the industry.