We report the changes in device performance of flexible amorphous indium-gallium-zinc-oxide thin-film transistors (TFTs) by 1.65% tensile or compressive bending stress for 10 k times. The TFTs exhibit negative threshold voltage (ΔV Th ) shift and enhanced drain current (I D ). TFT performance under repetitive tensile bending stress exhibits comparatively large threshold voltage shift (ΔV Th = -2.3 V) than compressive bending stress (ΔV Th = -0.9 V), which might be originated from both the generation of interface states (Nint) and gap trap density (dN gap /dE) by 3.5 × 10 11 /cm 2 and 5.7 × 10 12 /cm 2 eV, respectively under tensile bending stress. These are much higher than those (N int : 1.2 × 10 11 /cm 2 and dN gap /dE: 2.2 × 10 12 /cm 2 eV) for compressive bending. The increase in the DOS appears after both types of the bending stress which is related to the generation of oxygen vacancies. According to technology computer aided design simulation, the 10 k times repetitive compressive bending stress generates donor like states (ΔN GD ) ~ 2 × 10 16 cm -3 and tensile bending stress generates ΔN GD ~ 9.5 × 10 16 cm -3 at ~E C - 0.35 eV.
We report the numerical simulation of the effect of a dual gate (DG) TFT structure operating under dual gate driving on improving negative bias illumination stress (NBIS) of amorphous indium gallium zinc oxide thin-film transistors (a-IGZO TFTs). With respect to the transfer characteristics of a-IGZO TFTs, we show a larger negative threshold voltage shift (ΔVTH) with increasing a-IGZO active layer thickness. This trend is confirmed by TCAD simulation, where the initial transfer curve is plotted under varying a-IGZO thickness keeping a constant density of states. Under varying a-IGZO thickness, TCAD simulation results confirm TFTs under DG driving shows significantly less ΔVTH shift under NBIS compared with that of single gate (SG) driving TFTs. Under 10 K seconds of NBIS, TCAD simulation results show the increase in donor-like states (NGD) by 5.25 × 10 17 cm -3 eV -1 and acceptor-like states (NGA) by 7.5 × 10 16 cm -3 eV -1 .
29 July 2021 in ACS Applied Materials & Interfaces
We report a highly stable, nanocrystalline, zinc oxide (ZnO) thin-film transistor (TFT) fabricated by spray pyrolysis using purified ZrOₓ as a gate insulator. The crystalline ZnO layer shows an average grain size of 30 nm and a smooth surface with an average rms roughness value of 1.21 nm. The smoothness of the ZnO film is due to the alignment of all grains with the (002) c-axis. The TFTs exhibit a saturation mobility of 12.76 cm²/V· s, a subthreshold swing of 260 mV/dec, and an on/off current ratio of ~10⁸ with negligible hysteresis voltage. The ZnO TFT shows excellent stability under bias stress because of the high-quality ZnO film and its excellent interface with ZrOₓ. The conduction band tail width of ZnO was obtained from the TCAD fitting to the measurement data and was found to be 65 meV.
We investigate the effect of offset between source/drain (S/D) and gate electrodes (both top gate (TG) and bottom gate (BG)) on the electrical performance of dual-gate (DG) amorphous indium-gallium-zinc-oxide (a-IGZO) thin-film transistors (TFTs). The performance of the fabricated TFTs measured by BG sweep under various TG potentials are well fitted by TCAD simulation with the same density of states, which does not change with the device structure. The field-effect mobility is 15.5 cm 2 /Vs for the TFT with overlapped S/D electrodes, but it is less than 1 cm 2 /Vs for the offset TFTs. The low carrier concentration of ~10 16 cm -3 at the offset a-IGZO region is achieved by TCAD simulation, which increases the contact resistance, and thus induces current crowding and lower mobility in DG offset TFTs.
We report the effect of repeated tensile bending on the performance of amorphous indium-gallium- zinc oxide (a-IGZO) thin-film transistors (TFTs) on 15-μm polyimide substrate. Bending direction is vertical or parallel to the current path in a-IGZO TFT. With increasing bending time, the transfer curve shifts to the negative gate voltage direction. It is noted that the shift is smaller for longer channel length TFT. We performed technology computer aided design simulation for the TFT transfer curves and found that donorlike and acceptorlike states increase, respectively,by 2.5×10 17 and 0.4×10 17 cm -3 after 10k bending. The recovery of the transfer curve is studied by thermal annealing of the stressed TFT as a variation of annealing temperature and it is found that the performance can be completely recovered by thermal annealing at 300 °C for 1 h.