FATIMAH DE'NAN

Dr. FATIMAH DE'NAN

Universiti Sains Malaysia (USM)
orcid

Research Focus & Metrics

Academic Career Length

16Years (2011-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
2 November 2017 in Engineering Heritage Journal
Verified
Journal Article
Closed access
FATIMAH DE'NANFATIMAH DE'NAN
FATIMAH DE'NAN
Fadzli Mohamed NazriFadzli Mohamed Nazri
Fadzli Mohamed Nazri
NHNor Salwani Hashim
Nor Salwani Hashim

14 June 2022 in Polymers
Verified
Journal Article
Open access
PDF file
SSSrimala Sreekantan
Srimala Sreekantan
AYAng Xue Yong
Ang Xue Yong
NBNorfatehah Basiron
Norfatehah Basiron
FAFauziah Ahmad
Fauziah Ahmad
FATIMAH DE'NANFATIMAH DE'NAN
FATIMAH DE'NAN
Superhydrophobic coatings are widely applied in various applications due to their water-repelling characteristics. However, producing a durable superhydrophobic coating with less harmful low surface materials and solvents remains a challenge. Therefore, the aim of this work is to study the effects of three different solvents in preparing a durable and less toxic superhydrophobic coating containing polydimethylsiloxane (PDMS), silica solution (SS), and epoxy resin (DGEBA). A simple sol-gel method was used to prepare a superhydrophobic coating, and a spray-coating technique was employed to apply the superhydrophobic coating on tile substrates. The coated tile substrates were characterized for water contact angle (WCA) and tilting angle (TA) measurements, Field-Emission Scanning Electron Microscopy (FESEM), Atomic Force Microscopy (AFM), and Fourier Transform Infrared Spectroscopy (FTIR). Among 3 types of solvent (acetone, hexane, and isopropanol), a tile sample coated with isopropanol-added solution acquires the highest water contact angle of 152 ± 2° with a tilting angle of 7 ± 2° and a surface roughness of 21.80 nm after UV curing for 24 h. The peel off test showed very good adherence of the isopropanol-added solution coating on tiles. A mechanism for reactions that occur in the best optimized solvent is proposed.

1 January 2015 in Procedia Engineering
Verified
Journal Article
Open access
JLJin Ying Ling
Jin Ying Ling
SKShin Lin Kong
Shin Lin Kong
FATIMAH DE'NANFATIMAH DE'NAN
FATIMAH DE'NAN
Cold-formed C-channel steel purlins are widely used in construction industry. Since the cost of the steel is the main consideration in design, the concept of introducing web opening has been applied in the construction. A numerical study was undertaken to investigate the lateral-torsional buckling behaviour of cold-formed C-channel purlin with web opening. For this purpose a finite element model was developed using LUSAS software. It was then used in a detailed parametric study to simulate the lateral-torsional buckling and capacity of cold-formed steel purlins under varying perforated conditions. Five different shapes of opening were established to investigate the shape that gives the least reduction in buckling moment. Opening in the form of C-hexagon opening shape was used to develop models with different edge distance, different numbers of openings, different opening spacing and also different size of openings. For 3 m span, 0.5D opening size, where D is 175 mm, 750 mm edge distance with a total number of 13 openings with spacing 125 mm is found to reduce buckling moment by 3.56% but at the same time reducing the volume of the section by 5.16%. For the same span, edge distance, number of openings and spacing with 0.75D opening size, buckling moment reduced significantly by 9.16% while volume reduction by 11.61%. For all different size of openings, spacing and edge distance, the deformation pattern are similar. In conclusion, perforation do affects the buckling moment capacity of the C-channel purlin.

10 May 2022 in World Journal of Engineering
Verified
Journal Article
Closed access
FATIMAH DE'NANFATIMAH DE'NAN
FATIMAH DE'NAN
MJMegat Azmi Megat Johari
Megat Azmi Megat Johari
SNShaneez Christie Anak Nyandau
Shaneez Christie Anak Nyandau
NHNor Salwani Hashim
Nor Salwani Hashim
Purpose: The purpose of this study is to know the influence of palm oil fuel ash and metakaolin on the strength of concrete and crack resistance of reinforced concrete beam. An ordinary portland cement has been used in the concretes production where it is an important material to be considered due to its nature that reacts with every substance present. During the cement production, a significant amount of carbon dioxide is emitted from the clinker in rotary kiln and lot of energy is required in the production processes. Such an event can be prevented by replacing the part of cement with metakaolin (MK) and palm oil fuel ash (POFA). Aside from being a cementitious alternative, the materials can also contribute to a greener environment and more sustainable building, as POFA is available in Malaysia and may be used to substitute cement and minimize pollution. Design/methodology/approach: This study assesses the effect of MK and POFA on the concrete in terms of compressive strength and cracks pattern of the reinforced concrete beam based on the relevant previous studies. Findings: From this study, the compressive strength of concrete containing MK and POFA was higher than the control mix with the percentage of improvement in the range of 0.8%–78.2% for MK and 0.5%–14%, respectively. The optimum content of MK and POFA is between the range of 10% and 15% and 10% and 20%, respectively, to achieve high strength of concrete. Other than that, the inclusion of MK to the concrete mix improves the strength of reinforced concrete beams and reduces cracks on the surface of reinforced concrete beams, whereas the inclusion of POFA to the concrete mix increases the cracks on reinforced concrete beams. The cracks appeared within the flexure zone of every beam containing the MK and POFA. Originality/value: It was found that the fineness of MK and POFA has a significant influence on the mechanical properties of concrete.

14 June 2012 in Journal of Reinforced Plastics and Composites
Verified
Journal Article
Closed access
PDF file
JJJayapriya Jayaprakash
Jayapriya Jayaprakash
EPEmad Pournasiri
Emad Pournasiri
FATIMAH DE'NANFATIMAH DE'NAN
FATIMAH DE'NAN
This paper aims to investigate the effect of bond strength of corroded steel rebar embedded in concrete cylinders enveloped externally using hybrid and non-hybrid fiber reinforced polymer (FRP) reinforcement. A series of 16 concrete cylinders (i.e. 100 mm × 200 mm) embedded with steel rebar were prepared in the laboratory condition. The test variables were types of fiber reinforced polymer wrapping (i.e. hybrid and non-hybrid fiber reinforced polymer reinforcement), duration of corrosion activity, and percentage of mass loss in steel rebar. The specimens were immersed in 5% NaCl solution at a depth of 170 mm and anodic current was impressed through the rebar for accelerating the corrosion activity. After the exposure period of 24 days, the embedded steel rebar in concrete cylinder was pulled out monotonically to failure. The bond strength, percentage of mass loss in embedded steel rebar, and effect of different periods of corrosion activity on concrete cylinders enveloped with hybrid and non-hybrid fiber reinforced polymer reinforcement are addressed. Test results show that the observed bond strength of hybrid fiber reinforced polymer confined specimens was the highest as compared to the non-hybrid CFRP and GFRP confined specimens. Moreover, the bond strength performance of hybrid FRP confined specimens was slightly better than the non-hybrid CFRP confined specimens.

8 August 2014 in Journal of Composite Materials
Verified
Journal Article
Closed access
JJJayapriya Jayaprakash
Jayapriya Jayaprakash
EPEmad Pournasiri
Emad Pournasiri
FATIMAH DE'NANFATIMAH DE'NAN
FATIMAH DE'NAN
MAMp Anwar
Mp Anwar
The paper presents the effect of corrosion-damaged reinforced concrete (RC) columns with circular cross section enveloped (i.e. wrapped) with externally bonded hybrid and non-hybrid fibre-reinforced polymer (FRP) reinforcement. This study consisted of 18 RC circular columns with a diameter and height of 130 mm and 780 mm, respectively. These specimens were divided into three divisions, namely (i) no corrosion, (ii) mild corrosion and (iii) severe corrosion activities. All the mild and severe corroded columns, except control column, were exposed to corrosion activity, repaired with FRP and tested under eccentric loading. However, the columns without any corrosion activity were enveloped with FRP reinforcement and tested under eccentric loading. The corrosion process in RC columns was accelerated by impressing direct current on the steel reinforcement cage, adding 5% of NaCl in concrete mixture and wet/dry cycles. The variables investigated were different period of corrosion levels, plies of FRP (carbon and glass) reinforcement, hybrid (i.e. combination of carbon and glass FRP plies) and non-hybrid FRP (i.e. carbon or glass) reinforcement. From the experimental results, it was found that the external FRP confinement significantly increased the load-carrying capacity of the corrosion-damaged RC circular columns by 8% to 36% for mild corrosion level and 21% to 34% for severe corrosion level over the unconfined corrosion-damaged RC circular columns. Moreover, the results show that the performance of corrosion-damaged RC circular columns enveloped with hybrid FRP was better over the non-hybrid CFRP and GFRP RC circular columns. However, the results of CFRP enveloped circular columns were close to the hybrid FRP strengthened circular columns.