Fiber-reinforced asphalt concrete (FRAC) was tested using limestone, PG 64-22 binder, and 20% reclaimed asphalt pavement (RAP). After mixing fibers with different lengths and dosages, they were extracted and recovered to evaluate their dispersion in the FRAC. The uniaxial fatigue test, IDEAL CT test, and flow number test were performed on FRAC with different fiber lengths and asphalt contents. The balanced mix design (BMD) approach was then used to analyze the uniaxial and flow number test results in order to evaluate the effect of aramid fibers on fatigue and rutting resistance of the pavement. The dispersion test showed that the 19 mm and 10 mm aramid fibers at a dosage rate of 0.5 g/kg provided the best dispersion. The 19 mm fibers showed better performance test results than the 10 mm and 38 mm fibers. The BMD approach provided ranges of asphalt contents to produce mixes with certain resistances to fatigue and rutting. The BMD approach also demonstrated the effect of fibers with different lengths on increasing the resistance to fatigue and rutting. The study concluded that the 19 mm fibers with a dosage of 0.5 g/kg produce best results. The BMD approach is a good tool that can be used to refine the mix ingredients, including additives such as fibers, in order to optimize pavement resistance to various distresses such as fatigue cracking and rutting.
5 June 2023 in International Journal of Pavement Research and Technology
Published studies generally demonstrate positive benefits from using Mechanically Fibre-Reinforced Asphalt Concrete (M-FRAC). However, improvements vary with the particular asphalt mixture used in previous studies. The specific objectives of this study were to evaluate the mechanical properties of various asphalt mix designs reinforced with and without aramid fibres, to identify and quantify the key factors in the composition of asphalt mixtures that facilitate to the reinforcement mechanism of fibres, and finally associate the effect of asphalt mixture constituents on laboratory modulus, rutting and fatigue performance of M-FRAC. A total of seven different asphalt mix designs from across the United States were used in this study. For each mixture a non-fibre-reinforced variant and an M-FRAC variant were created and compared. Results showed that while overall fibres can improve the mechanical performance of asphalt mixtures, the degree of improvement varies from one mix to another. Further analysis and interpretation of the mixtures constituents revealed that there is a strong link between fibre reinforcement efficiency and composition of the asphalt mixtures. In particular, it was found that the effective binder content and gradation of the asphalt mixtures are good indicators of the likely performance benefit of M-FRAC with respect to rutting and fatigue cracking, respectively.
Asphalt aging is one of the main factors causing asphalt pavements deterioration. Previous studies reported on some aging benefits of asphalt rubber mixtures through laboratory evaluation. A field observation of various pavement sections of crumb rubber modified asphalt friction courses (ARFC) in the Phoenix, Arizona area indicated an interesting pattern of transverse/reflective cracking. These ARFC courses were placed several years ago on existing jointed plain concrete pavements for highway noise mitigation. Over the years, the shoulders had very noticeable and extensive cracking over the joints; however, the driving lanes of the pavement showed less cracking formation in severity and extent. The issue with this phenomenon is that widely adopted theories that stem from continuum mechanics of materials and layered mechanics of pavement systems cannot directly explain this phenomenon. One hypothesis could be that traffic loads continually manipulate the pavement over time, which causes some maltenes (oils and resins) compounds absorbed in the crumb rubber particles to migrate out leading to rejuvenation of the mastic in the asphalt mixture. To investigate the validity of such a hypothesis, an experimental laboratory testing was undertaken to condition samples with and without dynamic loads at high temperatures. This was followed by creep compliance and indirect tensile strength testing. The results showed the higher creep for samples aged with dynamic loading compared to those aged without loading. Higher creep compliance was attributed to higher flexibility of samples due to the rejuvenation of the maltenes. This was also supported by the higher fracture energy results obtained for samples conditioned with dynamic loading from indirect tensile strength testing.
23 September 2026 in Road Materials and Pavement Design
1. Road pavements are subject to progressive deterioration due to traffic loading, environmental exposure, and material aging. If not addressed in a timely manner, this deterioration can rapidly pr...
5 June 2026 in Construction and Building Materials