The majority of the published bio-based benzoxazine research has focused almost exclusively on different phenolic and amine compounds, while the aldehyde portion of the oxazine ring remains the same. These materials have been labeled as fully bio-based even though only two of the three raw materials are derived from renewable resources. In this study, we synthesize a truly bio-based benzoxazine in which all three reactants necessary to synthesize a benzoxazine are from renewable sources for the first time. The bio-originated compounds sesamol, furfurylamine, and benzaldehyde are used to synthesize a truly bio-based benzoxazine by a solventless method. Unlike almost all 1,3-benzoxazine resins reported in the literature thus far, the current paper reports oxazine ring-substituted benzoxazines, further providing a great opportunity for the molecular design flexibility of benzoxazine resins over the already very rich variation of 1,3-benzoxazine compounds. The structure of the 7-(furan-2-ylmethyl)-6,8-diphenyl-7,8-dihydro-6H-[1,3]dioxolo[4′,5′:3,4]benzo[1,2-e][1,3]oxazine monomer is characterized by Fourier transform infrared (FT-IR) spectroscopy, Raman spectroscopy, and 1D and 2D 1H and 13C nuclear magnetic resonance spectroscopy. The polymerization behavior of the benzoxazine monomer is studied by differential scanning calorimetry (DSC), and the thermal stability of the polybenzoxazine is evaluated by thermogravimetric analysis (TGA). The corresponding polymer has a high thermal stability with 5% and 10% weight loss temperatures of 317 and 332 °C, respectively, a char yield of 46%, and a heat release capacity of 201 J g−1 k−1. Polymers that show a high char yield, a high degradation temperature and a heat release capacity below 300 kJ g−1 are considered good anti-flammable materials.
An atomic-oxygen-erosion-resistant fluorinated benzoxazine resin and composite were developed. The benzoxazine resin, abbreviated as “BAF-oda-fu,” consists of four benzoxazine rings, and was synthesized from bisphenol AF (BAF), 4,4′-oxydianiline (oda), furfurylamine (fu), and paraformaldehyde. The resin was characterized by infrared spectroscopy (FT-IR), proton nuclear magnetic resonance spectroscopy (1H NMR), differential scanning calorimetry (DSC), and thermogravimetric analysis (TGA). An analysis of the solvent-washed product showed a technical grade purity (>95%) and a yield of approximately 85%. Subsequent polymerization of the resin was successfully performed by heating step-wise and opening the benzoxazine rings to form a crosslinked network. Thermal analyses showed a melting temperature of 115 °C and polymerization temperature of 238 °C, both being characteristic values of benzoxazine monomers. The benzoxazine resin was also blended with polyoctahedral sisesquoxane (POSS) and reinforced with alumina fibers. The Tg of the resin, as determined by DMA of the composite, could reach as high as 308 °C when post-curing and the POSS additive were utilized. The low-Earth orbit atomic-oxygen erosion rate was simulated by an RF plasma asher/etcher. The atomic-oxygen resistance of poly(BAF-oda-fu) fell along an established trend line based on its fluorine content.
A nacre-mimetic brick-and-mortar structure was used to develop a new flame-retardant technology. A second biomimetic approach was utilized to develop a non-flammable elastomeric benzoxazine for use as a polymer matrix that effectively adheres to the hydrophilic laponite nanofiller. A combination of laponite and benzoxazine is used to apply an ultra-high nanofiller content, thin nanocomposite coating on a polyurethane foam. The technology used is made environmentally friendly by eliminating the need to add any undesirable flame retardants, such as phosphorus additives or halogenated compounds. The very-thin coating on the polyurethane foam (PUF) is obtained through a single dip-coating. The structure of the polymer has been confirmed by proton nuclear magnetic resonance spectroscopy (1H NMR) and Fourier transform infrared spectroscopy (FTIR). The flammability of the polymer and nanocomposite was evaluated by heat release capacity using microscale combustion calorimetry (MCC). A material with heat release capacity (HRC) lower than 100 J/Kg is considered non-ignitable. The nanocomposite developed exhibits HRC of 22 J/Kg, which is well within the classification of a non-ignitable material. The cone calorimeter test was also used to investigate the flame retardancy of the nanocomposite’s thin film on polyurethane foam. This test confirms that the second peak of the heat release rate (HRR) decreased 62% or completely disappeared for the coated PUF with different loadings. Compression tests show an increase in the modulus of the PUF by 88% for the 4 wt% coating concentration. Upon repeated modulus tests, the rigidity decreases, approaching the modulus of the uncoated PUF. However, the effect of this repeated mechanical loading does not significantly affect the flame retarding performance.