Ethylene–vinyl acetate copolymer (EVA), a crucial elastomeric resin, finds extensive application in the footwear industry. Conventional chemical foaming agents, including azodicarbonamide and 4,4′-oxybis(benzenesulfonyl hydrazide), have been identified as environmentally problematic. Hence, this study explores the potential of physical foaming of EVA using supercritical nitrogen as a sustainable alternative, garnering considerable interest in both academia and industry. The EVA formulations and processing parameters were optimized and EVA foams with densities between 0.15 and 0.25 g/cm3 were produced. Key findings demonstrate that physical foaming not only reduces environmental impact but also enhances product quality by a uniform cell structure with small cell size (50–100 μm), a wide foaming temperature window (120–180 °C), and lower energy consumption. The research further elucidates the mechanisms of cell nucleation and growth within the crosslinked EVA network, highlighting the critical role of blowing agent dispersion and localized crosslinking around nucleated cells in defining the foam’s cellular morphology. These findings offer valuable insights for producing EVA foams with a more controllable cellular structure, utilizing physical foaming techniques.
The diverse physical appearances and wide density range of polymer bead foams offer immense potential in various applications and future advancements. The multiscale and multilevel structural features of bead foams involve many fundamental scientific topics. This review presents a comprehensive overview of recent progress in the preparation and molding techniques of bead foams. Firstly, it gives a comparative analysis on the bead foam characteristics of distinct polymers. Then, a summary and comparison of molding techniques employed for fabricating bead foam parts are provided. Beyond traditional methods like steam-chest molding (SCM) and adhesive-assisted molding (AAM), emerging techniques like in-mold foaming and molding (IMFM) and microwave selective sintering (MSS) are highlighted. Lastly, the bonding mechanisms behind these diverse molding methods are discussed.
High-hardness thermoplastic polyurethane (HD-TPU) presents a high matrix modulus, low-temperature durability, and remarkable abrasion resistance, and has been used in many advanced applications. However, the fabrication of microcellular HD-TPU foam is rarely reported in the literature. In this study, the foaming behavior of HD-TPU with a hardness of 75D was investigated via a pressure-quenching foaming process using CO2 as a blowing agent. Microcellular HD-TPU foam with a maximum expansion ratio of 3.9-fold, a cell size of 25.9 μm, and cell density of 7.8 × 108 cells/cm3 was prepared, where a high optimum foaming temperature of about 170 °C had to be applied with the aim of softening the polymer’s matrix modulus. However, the foaming behavior of HD-TPU deteriorated when the foaming temperature further increased to 180 °C, characterized by the presence of coalesced cells, microcracks, and a high foam density of 1.0 g/cm3 even though the crystal domains still existed within the matrix. The cell morphology evolution of HD-TPU foam was investigated by adjusting the saturation time, and an obvious degradation occurred during the high-temperature saturation process. A cell growth mechanism of HD-TPU foams in degradation environments was proposed to explain this phenomenon based on the gas escape through the defective matrix.
Poly (butylene adipate-co-terephthalate) (PBAT) foam sheets prepared by foaming supercritical fluids are characterized by high resilience, homogeneous cellular structure, and well-defined biodegradability. However, the inert chemical structure and the rigid hard segments restrict the diffusion of CO2 within the PBAT matrix, resulting in extremely long gas saturation times as long as 9 h at a thickness of 12 mm. In this study, microporous structures were pre-introduced into the PBAT matrix to provide a fast gas diffusion pathway during the saturation process. After 2 h of saturation, PBAT foam sheets with expansion ratio of 10 to 13.8 times were prepared. The interaction of CO2 with PBAT was systematically investigated, and the CO2 sorption process was evaluated kinetically and thermodynamically using the Fickian diffusion theory. The solubility and diffusion rate of CO2 in pretreated PBAT sheets with different microporous sizes and densities were investigated, and the effects of pretreatment strategies on the foaming behavior and cell structure of PBAT foam sheets were discussed. The introduction of a microporous structure not only reduces saturation time but also enhances solubility, enabling the successful preparation of soft foams with high expansion ratios and resilience. After undergoing foaming treatment, the PBAT pretreated sheets with a 10 μm microporous structure and a density of 0.45 g/cm3 demonstrated improved mechanical properties: their hardness decreased to 35 C while resilience increased to 58%, reflecting enhanced elastic recovery capabilities. The pretreatment method, which increases the diffusion rate of CO2 in PBAT sheets, offers a straightforward approach that provides valuable insights into achieving rapid and efficient foaming of thick PBAT sheets in industrial applications.