The synthesis of hydrogel beads involving natural polymers is, nowadays, a leading research area. Among natural polymers, starch and chitosan represent two biomolecules with proof of efficiency and low economic impact in various utilization fields. Therefore, herein, the features of hydrogel beads obtained from chitosan and three sorts of starch (potato, wheat and rise starches), grafted with acrylonitrile and then amidoximated, were deeply investigated for their use as sorbents for heavy metal ions and dyes. The hydrogel beads were prepared by ionotropic gelation/covalent cross-linking of chitosan and functionalized starches. The chemical structure of the hydrogel beads was analyzed by FT-IR spectroscopy; their morphology was revealed by optical and scanning electron microscopies, while the influence of the starch functionalization strategies on the crystallinity changes was evaluated by X-ray diffraction. Molecular dynamics simulations were used to reveal the influence of the grafting reactions and grafted structure on the starch conformation in solution and their interactions with chitosan. The sorption capacity of the hydrogel beads was tested in batch experiments, as a function of the beads’ features (synthesis protocol, starch sort) and simulated polluted water, which included heavy metal ions (Cu2+, Co2+, Ni2+ and Zn2+) and small organic molecules (Direct Blue 15 and Congo red).
A biological/synthetic hybrid graft copolymer was obtained by grafting poly(acrylic acid) (PAA, synthesized via reversible addition-fragmentation chain transfer (RAFT) polymerization) to amylopectin (AMP). The novel graft copolymer presents amphiphilic properties due to the inherent insolubility of AMP in water and was further utilized as a mediator for the synthesis of gold nanoparticles (AuNPs) following an environmentally friendly in situ procedure. The AMP-g-PAA copolymer formation by the interaction of the PAA end groups with the C(6)-OH groups on an AMP backbone was confirmed by Attenuated Total Reflectance-Fourier Transform Infrared (ATR-FTIR) and 1D (proton (1H NMR) and carbon (13C NMR) nuclear magnetic resonance, and Distortionless Enhancement by Polarization Transfer (DEPT)) and 2D (correlation (COSY) and heteronuclear single quantum coherence (HSQC)) spectroscopies. The calculated degree of substitution of 1.17 suggests that the grafting was done at one OH from the three in an anhydroglycosidic unit (AGU) (preferably at that in C6 position), with a mean grafting efficiency of 76%. Additional information obtained using thermogravimetric analysis shows that the thermal decomposition of AMP-g-PAA occurs in two steps, with a residual mass of ~16 wt% at 700 °C, higher than AMP or PAA, indicating increased thermal stability of the copolymer. Dynamic and electrophoretic light scattering (DLS and ELS) measurements were used to determine the hydrodynamic size and ionic charge of the AMP-g-PAA self-assemblies in aqueous solution as well as their stability. The AMP-g-PAA was subsequently tested as a reducing agent in the environmentally friendly synthesis of AuNPs in aqueous solution, at different incubation temperatures, reaction duration, and inorganic/polymer weight ratios. The development of the surface plasmon resonance band of AuNPs, observed in UV–vis spectra, was consistently monitored over the reaction time. DLS analysis indicated time-dependent changes in the AuNPs’ particle size distributions, while scanning transmission electron microscopy confirmed that the AuNPs formed at the inorganic/polymer weight ratio of 0.36 and at 60 °C were predominantly well-dispersed, spherical-shaped nanoparticles. The AuNPs synthesized in situ within the copolymer matrix did not introduce additional cytotoxicity compared to the parent copolymer alone, with the composites representing a promising safety baseline for further investigation in biomedical applications.