Herein, we report a novel approach to obtaining magnesium and nanocrystal Mg-Al alloy from magnesia using a closed microwave aluminothermic method in order to solve the problems of high energy consumption, high pollution, and low productivity in the process of magnesium and its alloy production. The main idea of the paper is to design a technique for the preparation of magnesium–aluminum alloy during the reduction process of MgO directly under atmospheric pressure. Based on this experimental idea, we have established a closed microwave aluminothermic reduction reactor. The great advantage of the reaction device is that it can make the reaction material heat up quickly to the reaction temperature in the microwave heating process and produce high-pressure magnesium vapor, which reacts with aluminum dramatically to form Mg-Al alloy under microwave irradiation. By the calculation of the electromagnetic field of the reaction device and sample using ANSYS electronics desktop 2018, the optimum microwave heating conditions for samples have been established. Based on the calculation results, we demonstrate that magnesium and its alloy are prepared successfully by using this method. In addition, the reduction rate of MgO is greatly improved, which is higher up to 79.97 Wt% when the reduction time is 30 min, at 1273 K, and the Mg2Al3 and MgAl alloy is formed during the reduction process as well. Moreover, the formation mechanism of Mg-Al alloy during the reduction process under microwave irradiation was discussed further. Our findings could provide a new approach, insights, and research directions to obtain magnesium and Mg-Al alloy directly from magnesia under normal pressure.
An HfC-doped molybdenum (Mo-Hf-C; MHC) alloy was prepared via a powder metallurgy process, including dry direct doping followed by ball-milling, cold-isotactic-pressing, and vacuum sintering. An oxidation comparison experiment was conducted, and the oxidation and volatilization behaviors were analyzed using the mass change, volatile generation rate, and morphology transformation. The results show that relatively uniform powder morphology can be obtained by the direct doping of carbide and high-energy ball milling. The oxidation of the MHC alloy at a lower temperature was characterized by the oxygen-absorption and a slight weight gain, while at a higher temperature and longer holding time, it was characterized by the mass volatile weight loss. A significant weight change appeared at 800 °C for 30 min with a weight loss rate of 4.8%. Surface oxidation products developed horizontally from ridged oxides at lower temperature stages to a flaky oxide layer at higher temperatures. The peeling of the oxide layer was the result of interfacial pore development, which led to exposure of the alloy matrix and further oxidation. Based on the oxidation and volatilization characteristics of HfC-doped MHC alloys, we conclude that the oxidation and volatilization of the MHC alloy conformed to the general law; however, the significant weight loss temperature, weight loss rate, volatilization temperature, and volatilization rate were improved compared with pure molybdenum and traditional molybdenum alloys, thus, indicating that the precipitation of the second phase HfC particles at the grain boundaries and within the grains can inhibit the oxidation and volatilization of matrix elements to a certain extent.