As the semiconductor industry has continuously reduced the integrated circuit (IC) chip size, a resistance-capacitance (RC) delay emerged, causing deterioration of the chip performance. To reduce the RC delay, low dielectric constant (low-k) films with suitable mechanical strengths have been adopted as intermetal dielectrics (IMDs). In this study, low-k plasma-polymerized diethoxymethylsilane (ppDEMS) films were fabricated by plasma-enhanced chemical vapor deposition of the DEMS precursor with a flow rate ratio of the DEMS precursor to helium (He) carrier gas (DEMS/He FRR) as a key parameter. As the DEMS/He FRR increased, the refractive index was reduced from 1.401 to 1.386, and the k value decreased from 2.77 to 2.10. From high-resolution scans of C1s, O1s, and Si2p peaks of X-ray photoelectron spectroscopy, the carbon contents increased, and the oxygen contents decreased, along with a decrease in the film density. With the increased DEMS/He FRR, hardness decreased from 2.5 to 1.8 GPa, and elastic modulus decreased from 17.08 to 11.50 GPa. Leakage current densities for all the ppDEMS films were less than 10−7 A cm−2 at 1 MV cm−1. The ppDEMS films could be suggested as the IMDs according to their electrical and mechanical performance.
As semiconductor chips have been integrated to enhance their performance, a low-dielectric-constant material, SiCOH, with a relative dielectric constant k ≤ 3.5 has been widely used as an intermetal dielectric (IMD) material in multilevel interconnects to reduce the resistance-capacitance delay. Plasma-polymerized tetrakis(trimethylsilyoxy)silane (ppTTMSS) films were created using capacitively coupled plasma-enhanced chemical vapor deposition with deposition plasma powers ranging from 20 to 60 W and then etched in CF4/O2 plasma using reactive ion etching. No significant changes were observed in the Fourier-transform infrared spectroscopy (FTIR) spectra of the ppTTMSS films after etching. The refractive index and dielectric constant were also maintained. As the deposition plasma power increased, the hardness and elastic modulus increased with increasing ppTTMSS film density. The X-ray photoelectron spectroscopy (XPS) spectra analysis showed that the oxygen concentration increased but the carbon concentration decreased after etching owing to the reaction between the plasma and film surface. With an increase in the deposition plasma power, the hardness and elastic modulus increased from 1.06 to 8.56 GPa and from 6.16 to 52.45 GPa. This result satisfies the hardness and elastic modulus exceeding 0.7 and 5.0 GPa, which are required for the chemical–mechanical polishing process in semiconductor multilevel interconnects. Furthermore, all leakage-current densities of the as-deposited and etched ppTTMSS films were measured below 10−6 A/cm2 at 1 MV/cm, which is generally acceptable for IMD materials.
Biliary stents are medical devices inserted into the bile duct to treat biliary strictures. However, inserted stents can become occluded within a few months after placement. In this study, the inner surface of a polyethylene (PE) tube was plasma-treated with helium (He), nitrogen (N2), oxygen (O2), and their gas mixtures to improve resistance to stent occlusion. Surface characteristics were analyzed by water contact angle (WCA) and x-ray photoelectron spectroscopy (XPS) measurements. In the WCA results, bare PE without plasma treatment was the most hydrophobic at 100.7°, whereas PE(He) plasma-treated with He gas became the most hydrophilic at 26.1°. XPS deconvolution analysis revealed that the PE(He) and PE(He/N2) contained a considerable proportion of O 1s present as amide (–CONH–) groups exceeding 40%, whereas the other samples had proportions below 7%. The resistance to stent occlusion was verified through microbial and cancer cell adhesion assays. In the microbial adhesion assay, Escherichia coli (E. coli) was used, and PE(He) showed a statistically significant reduction in E. coli growth compared to bare PE. Inhibition of cancer cell adhesion was the most pronounced in PE(He) and PE(He/N2), with reductions in fluorescence intensities of 75.5% and 81.5%, respectively. Overall, both surface hydrophilization and amidation were found to be effective in inhibiting the adhesion of organic contaminants. It was proposed that plasma surface treatment has the potential to improve resistance to biliary stent occlusion.