Nedjima Bouzidi

Prof. Nedjima Bouzidi


Research Focus & Metrics

Academic Career Length

9Years (2018-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
16 April 2024 in Materials
Verified
Journal Article
Open access
PDF file
Sergio Martinez-MartinezSergio Martinez-Martinez
Sergio Martinez-Martinez
KBKarima Bouguermouh
Karima Bouguermouh
Nedjima BouzidiNedjima Bouzidi
Nedjima Bouzidi
LMLaila Mahtout
Laila Mahtout
Sánchez Soto Pedro JoséSánchez Soto Pedro José
Sánchez Soto Pedro José
Luis Pérez-VillarejoLuis Pérez-Villarejo
Luis Pérez-Villarejo
In the present work, the development of geopolymeric materials with Na or K based on industrial kaolin samples, with variable kaolinite content and alkaline silicates, is studied. XRF, XRD, FTIR and SEM-EDS have been used as characterization techniques. Three ceramic kaolin samples, two from Algeria and one from Charente (France), have been considered. In particular, chemical and mineralogical characterization revealed elements distinct of Si and Al, and the content of pure kaolinite and secondary minerals. Metakaolinite was obtained by grinding and sieving raw kaolin at 80 μm and then by thermal activation at 750 °C for 1 h. This metakaolinite has been used as a base raw material to obtain geopolymers, using for this purpose different formulations of alkaline silicates with NaOH or KOH and variable Si/K molar ratios. The formation of geopolymeric materials by hydroxylation and polycondensation characterized with different Si/Al molar ratios, depending on the original metakaolinite content, has been demonstrated. Sodium carbonates have been detected by XRD and FTIR, and confirmed by SEM-EDS, in two of these geopolymer materials being products of NaOH carbonation.

1 September 2018 in Clay Minerals
Verified
Journal Article
Closed access
PDF file
Nedjima BouzidiNedjima Bouzidi
Nedjima Bouzidi
ABAthmane Bouzidi
Athmane Bouzidi
RNRaphael Oliveira Nunes
Raphael Oliveira Nunes
DMDjoudi Merabet
Djoudi Merabet
The present study examined the microstructure and mechanical properties of ceramic composites based on a kaolin from Djebel Debbagh, northeast Algeria, composed mainly of kaolinite and halloysite with the addition of various amounts of BaCO3. The composites were prepared by high-energy ball milling and sintered at 1100°C and 1200°C for 3 h. The samples sintered at 1200°C without BaCO3were composed mainly of mullite, which disappeared with increasing BaCO3content. X-ray diffraction investigation showed the presence of hexacelsian (BaAl2SiO6and BaAl2Si2O8), which disappeared at BaCO3contents >50 wt.% in favour of barium aluminium and barium silicate phases. At 40 wt.% BaCO3content, the porosity of the composites decreased from 0.7% to 0.1% and the microhardness increased from 7 to 8 GPa, respectively, at 1100°C and 1200°C due to the amorphous phase.

1 September 2025 in Clay Minerals
Verified
Journal Article
Open access
PDF file
HBHadjer Bouzeriba
Hadjer Bouzeriba
Nedjima BouzidiNedjima Bouzidi
Nedjima Bouzidi
AIAbdelaziz Idres
Abdelaziz Idres
ILImen Laala
Imen Laala
FMFarid Ait Merzeg
Farid Ait Merzeg
Iron mining waste is produced from the iron ore mining operations of El Ouenza Mine (north-east Algeria), and it is not currently recycled to preserve the environment. The current study aims at developing sustainable clay bricks by mixing clay with different proportions of iron mining waste (ranging from 10 to 50 wt.%) and fired at 850°C and 950°C. Addition of 30 wt.% Iron mining waste had a positive effect on the physical and mechanical properties of the fired clay bricks. Linear shrinkage, water absorption and porosity were reduced, while compressive and flexural strengths were increased. Furthermore, up to 30 wt.% of iron mining waste addition to the mixtures improved compressive and flexural strengths to 59.17 and 10.06 MPa, respectively, when the bricks were fired at 950°C. According to their thermal conductivity, the bricks with 10–50 wt.% iron mining waste are considered as thermal insulators, with thermal conductivity values ranging from 0.45 to 0.56 W m –1 K –1 . Adding 30 wt.% of iron mining waste can lead to the production of eco-friendly bricks with high mechanical and thermal properties, generating economic and environmental benefits.