In this paper, we analyze the influence of Al doping on microstructure and light emission efficiency of ZnO nanoparticles obtained by the hydrothermal method and after vapor condensation method, where vaporization of the precursor powders was caused by high solar energy and subsequent deposition. We report an increase of lattice parameters with increasing level of doping as well as large emission enhancement, which we relate to surface passivation of recombination mechanisms and/or plasmon mechanism of photoluminescence stimulation.
The aim of this work was to study the effect of the applied chemical reaction stimulation method on the morphology and structural properties of zinc oxide nanoparticles (ZnONPs). Various methods of chemical reaction induction were applied, including microwave, high potential, conventional resistance heater and autoclave-based methods. A novel, high potential-based ZnONPs synthesis method is herein proposed. Structural properties–phase purity, grain size–were examined with XRD methods, the specific surface area was determined using BET techniques and the morphology was examined using SEM. Based on the results, the microwave and autoclave syntheses allowed us to obtain the desired phase within a short period of time. The impulse-induced method is a promising alternative since it offers a non-equilibrium course of the synthesis process in an highly energy-efficient manner.
The drawback of the hydrothermal technique is driven by the fact that it is a time-consuming operation, which greatly impedes its commercial application. To overcome this issue, conventional hydrothermal synthesis can be improved by the implementation of microwaves, which should result in enhanced process kinetics and, at the same time, pure-phase and homogeneous products. In this study, nanometric zinc aluminate (ZnAl2O4) with a spinel structure was obtained by a hydrothermal method using microwave reactor. The average ZnAl2O4 crystallite grain size was calculated from the broadening of XRD lines. In addition, BET analysis was performed to further characterize the as-synthesized particles. The synthesized materials were also subjected to microscopic SEM and TEM observations. Based on the obtained results, we concluded that the grain sizes were in the range of 6–8 nm. The surface areas measured for the samples from the microwave reactor were 215 and 278 m2 g−1.