The development of a novel ironmaking technology based on fine iron ore concentrate in a flash reactor is summarized. The design of potential industrial reactors for flash ironmaking based on the computational fluid dynamics technique is described. Overall, this simulation work has shown that the size of the reactor used in the novel flash ironmaking technology (FIT) can be quite reasonable vis-à-vis the blast furnaces. A flash reactor of 12 m diameter and 35 m height with a single burner operating at atmospheric pressure would produce 1.0 million tons of iron per year. The height can be further reduced by either using multiple burners, preheating the feed gas, or both. The computational fluid dynamics (CFD)-based design of potential industrial reactors for flash ironmaking pointed to a number of features that should be incorporated. The flow field should be designed in such a way that a larger portion of the reactor is used for the reduction reaction but at the same time excessive collision of particles with the wall must be avoided. Further, a large diameter-to-height ratio that still allows a high reduction degree should be used from the viewpoint of decreased heat loss. This may require the incorporation of multiple burners and solid feeding ports.
Commercial polyurethane foam was treated with salicylate salt to synthesize PUFSalicylate (PUFS) as a novel, promising, stable and inexpensive adsorbent for chlorpyrifos (CPF) extraction. The properties of PUFS were investigated using UV–Vis spectroscopy, apparent density, FTIR spectroscopy, pHZPC, BET surface area, elemental analysis, TGA and DTG tests. Batch experiments were performed for the sorption of CPF under different salicylate concentrations, pH, shaking time, ionic strength, agitation speed, sorbent mass, batch factor and initial concentration of CPF. The results confirmed that 97.4% of CPF in a 25 mL solution, 10 μg/L concentration, could be retained by only 0.3 mg of PUFS (1:105mass ratio of PUFS: solution). In addition, the maximum capacity of PUFS for the sorption of CPF was 1249.8 μg/mg (3.9 × 10−5 mol/g) within 180 min. The negative values of ΔH° and ΔG° indicated that the sorption of CPF onto PUFS is an exothermic spontaneous process (favorable). The calculated data from the experimental procedures fitted perfectly with Freundlich isotherm (R2 = 0.9952) and the kinetic Equation of pseudo-second order. In addition, the R2 value in the Elovich Equation recorded higher when compared to the Morris–Weber and Bangham Equations; hence, the pore diffusion is not the rate-determining step. Thus, the use of PUFSalicylate for the removal of chlorpyrifos contaminations from agriculture runoff is applicable.
24 July 2020 in Metallurgical and Materials Transactions B