This research successfully enhances the mechanical properties of the ready-market resin product additively printed by using stereolithography (SLA) reinforced with glass powder. Using Esun Standard Resin (Shenzhen, China), various proportions of glass powder (0%, 1%, 2%, 3%, 4%, 5%, 10%, 15%, and 25%) were mixed to create test specimens. The results indicated that the incorporation of glass powder markedly enhanced tensile strength and hardness. Specimens containing 25% glass powder exhibited a tensile strength of 37.01 MPa and a hardness of 84.5 HV, in contrast to 24.03 MPa and 73.7 HV for those without glass powder. The density rose with the addition of glass powder, attaining 1.338 g/cm3 at 25% concentration. Nevertheless, heightened brittleness and reduced strain values signified a compromise between strength and ductility. Compression testing revealed increased maximum stress but more brittleness with higher glass powder content, while flexural testing demonstrated diminished flexural strength attributed to inadequate filler adherence and dispersion. This study highlights that the addition of glass powder to SLA resins can improve mechanical strength while reducing flexibility and ductility. Enhancing the concentration and dispersion of glass powder is crucial for attaining a balance in mechanical properties, which enhances SLA 3D printing for dependable, high-performance engineering applications.
The growing demand for complex structures, energy absorption, and mechanically strong materials has led to the exploration of innovative composites. This study focuses on the manufacture, characterization, and evaluation of PLA+ reinforced with woven glass fiber. Using Fused Filament Fabrication (FFF) 3D Printer technology, the effects of adding woven glass fiber were examined through a tensile test with Digital Image Correlation (DIC)-induced, flexural, Charpy impact resistance, Shore D hardness, Differential Scanning Calorimetry (DSC) thermal tester, and SEM morphological tests. Results showed that adding four layers of glass fiber significantly improved mechanical properties: tensile strength increased by 85% to 95.44 MPa, flexural strength by 13% to 91.51 MPa, and impact resistance by 450% to 15.12 kJ/m2. However, a reduction in hardness and thermal resistance was noted due to chemical interactions. These findings suggest potential applications of PLA+ composites in high-strength products for vehicle bumpers in the automotive industry and shin pads in the sports industry.