Spider silks are among the toughest known materials and thus provide models for renewable, biodegradable, and sustainable biopolymers. However, the entirety of their diversity still remains elusive, and silks that exceed the performance limits of industrial fibers are constantly being found. We obtained transcriptome assemblies from 1098 species of spiders to comprehensively catalog silk gene sequences and measured the mechanical, thermal, structural, and hydration properties of the dragline silks of 446 species. The combination of these silk protein genotype-phenotype data revealed essential contributions of multicomponent structures with major ampullate spidroin 1 to 3 paralogs in high-performance dragline silks and numerous amino acid motifs contributing to each of the measured properties. We hope that our global sampling, comprehensive testing, integrated analysis, and open data will provide a solid starting point for future biomaterial designs.
The development of artificial spider silk with properties similar to native silk has been a challenging task in materials science. In this study, we use a microfluidic device to create continuous fibers based on recombinant MaSp2 spidroin. The strategy incorporates ion-induced liquid-liquid phase separation, pH-driven fibrillation, and shear-dependent induction of β-sheet formation. We find that a threshold shear stress of approximately 72 Pa is required for fiber formation, and that β-sheet formation is dependent on the presence of polyalanine blocks in the repetitive sequence. The MaSp2 fiber formed has a β-sheet content (29.2%) comparable to that of native dragline with a shear stress requirement of 111 Pa. Interestingly, the polyalanine blocks have limited influence on the occurrence of liquid-liquid phase separation and hierarchical structure. These results offer insights into the shear-induced crystallization and sequence-structure relationship of spider silk and have significant implications for the rational design of artificially spun fibers.
Covalently cross-linked rubber materials are widely used in elastic applications due to their excellent mechanical properties. However, the irreversibility of covalent cross-linking suffers from poor material recyclability. As a degradable polypeptide-based cross-linker for polybutadiene, poly(l-cysteine) (polyCys) was synthesized via papain-catalyzed chemoenzymatic polymerization. The resulting polyCys had intact thiol groups that cross-linked polybutadiene via the thiol-ene reaction. The cross-linking reaction of polybutadiene was performed in the presence of polyCys and a radical initiator and resulted in insoluble polybutadiene gel formation. Based on Raman spectroscopy analysis, the cross-linking reaction was confirmed by the consumption of thiol groups of polyCys. From the dynamic viscoelastic analyses of the cross-linked polybutadienes, the viscoelasticity drastically changed from that of raw polybutadiene, with the disappearance of the slow relaxation mode at low frequencies. The complete network formation was confirmed by E′ and E′′ showing the power law over the whole frequency range, as determined by the time-course experiments of the dynamic viscoelastic properties. The cross-linked polybutadiene was degradable by acid hydrolysis, resulting in the regeneration of soluble polybutadiene. Polypeptide cross-linked polybutadiene materials are promising candidates for the application of polybutadiene-based rubber materials with the requirements of both material integrity and reusability.
Silk composites with natural rubber (NR) were prepared by mixing degummed silk and NR latex solutions. A significant enhancement of the mechanical properties was confirmed for silk/NR composites compared to a NR-only product, indicating that silk can be applied as an effective reinforcement for rubber materials. Attenuated total reflection Fourier transform infrared (ATR-FTIR) and wide-angle X-ray diffraction (WAXD) analysis revealed that a β-sheet structure was formed in the NR matrix by increasing the silk content above 20 wt%. Then, 3,4-dihydroxyphenylalanine (DOPA)-modified silk was also blended with NR to give a DOPA-silk/NR composite, which showed superior mechanical properties to those of the unmodified silk-based composite. Not only the chemical structure but also the dominant secondary structure of silk in the composite was changed after DOPA modification. It was concluded that both the efficient adhesion property of DOPA residue and the secondary structure change improved the compatibility of silk and NR, resulting in the enhanced mechanical properties of the formed composite. The knowledge obtained herein should contribute to the development of the fabrication of novel silk-based elastic materials.