High-performance Li-ion/metal batteries working at a low temperature (i.e., <−20 °C) are desired but hindered by the sluggish kinetics associated with Li+ transport and charge transfer. Herein, the temperature-dependent Li+ behavior during Li plating is profiled by various characterization techniques, suggesting that Li+ diffusion through the solid electrolyte interface (SEI) layer is the key rate-determining step. Lowering the temperature not only slows down Li+ transport, but also alters the thermodynamic reaction of electrolyte decomposition, resulting in different reaction pathways and forming an SEI layer consisting of intermediate products rich in organic species. Such an SEI layer is metastable and unsuitable for efficient Li+ transport. By tuning the solvation structure of the electrolyte with a lower lowest unoccupied molecular orbital (LUMO) energy level and polar groups, such as fluorinated electrolytes like 1 mol L−1 lithium bis(fluorosulfonyl)imide (LiFSI) in methyl trifluoroacetate (MTFA): fluoroethylene carbonate (FEC) (8:2, weight ratio), an inorganic-rich SEI layer more readily forms, which exhibits enhanced tolerance to a change of working temperature (thermodynamics) and improved Li+ transport (kinetics). Our findings uncover the kinetic bottleneck for Li+ transport at low temperature and provide directions to enhance the reaction kinetics/thermodynamics and low-temperature performance by constructing inorganic-rich interphases.
Fast-charging lithium-ion batteries are highly required, especially in reducing the mileage anxiety of the widespread electric vehicles. One of the biggest bottlenecks lies in the sluggish kinetics of the Li+ intercalation into the graphite anode; slow intercalation will lead to lithium metal plating, severe side reactions, and safety concerns. The premise to solve these problems is to fully understand the reaction pathways and rate-determining steps of graphite during fast Li+ intercalation. Herein, we compare the Li+ diffusion through the graphite particle, interface, and electrode, uncover the structure of the lithiated graphite at high current densities, and correlate them with the reaction kinetics and electrochemical performances. It is found that the rate-determining steps are highly dependent on the particle size, interphase property, and electrode configuration. Insufficient Li+ diffusion leads to high polarization, incomplete intercalation, and the coexistence of several staging structures. Interfacial Li+ diffusion and electrode transportation are the main rate-determining steps if the particle size is less than 10 μm. The former is highly dependent on the electrolyte chemistry and can be enhanced by constructing a fluorinated interphase. Our findings enrich the understanding of the graphite structural evolution during rapid Li+ intercalation, decipher the bottleneck for the sluggish reaction kinetics, and provide strategic guidelines to boost the fast-charging performance of graphite anode.
The emerging cryogenic electron microscopy (cryo-EM) has demonstrated its power and essential role in probing the beam-sensitive battery materials and delivering new insights. With the increasing interest in cryo-EM for battery materials and interfaces, herein we provide the strategies of obtaining fresh and native structural information with minimal artifacts, including sample preparation, transferring, imaging, and data interpretation. We summarize the recent achievements enabled by cryo-EM and point out some unsolved/potential questions in terms of the bulk materials, solid-solid interface, and solid-liquid interfaces of batteries. Finally, we conclude with perspectives on the future developments and applications of cryo-EM in battery materials and interfaces.
Lithium metal is a promising anode material for its low redox potential and high theoretical specific capacity. However, the commercial application of the lithium metal anode is hindered with safety concerns arising from the uncontrolled growth of the lithium dendrites and significant volume variation during the lithium plating and stripping processes. Modification to the current collector is effective in tailoring the morphology of the deposited lithium and improving the cycling performance of the lithium metal batteries This review summarizes at first the global research advances in the structural design and the selection of the current collectors and their textures. It then presents some of our efforts in realizing controlled lithium deposition by designing current collectors in three aspects, lithium deposition induced by the micro-to-nano structures, lithiophilic alloys and iron carbides. Finally, conclusions and prospects are made for the further research of the current collectors.