In this paper, the effects of Nb addition (5–20 wt %) on the microstructure, mechanical properties, corrosion behavior, and cytotoxicity of Ti-Nb alloys were investigated with the aim of understanding the relationship between phase/microstructure and various properties of Ti-xNb alloys. Phase/microstructure was analyzed using X-ray diffraction (XRD), SEM, and TEM. The results indicated that the Ti-xNb alloys (x = 10, 15, and 20 wt %) were mainly composed of α + β phases with precipitation of the isothermal ω phase. The volume percentage of the ω phase increased with increasing Nb content. We also investigated the effects of the alloying element Nb on the mechanical properties (including Vickers hardness and elastic modulus), oxidation protection ability, and corrosion behavior of Ti-xNb binary alloys. The mechanical properties and corrosion behavior of Ti-xNb alloys were found to be sensitive to Nb content. These experimental results indicated that the addition of Nb contributed to the hardening of cp-Ti and to the improvement of its oxidation resistance. Electrochemical experiments showed that the Ti-xNb alloys exhibited superior corrosion resistance to that of cp-Ti. The cytotoxicities of the Ti-xNb alloys were similar to that of pure titanium.
We performed a systematic investigation of the Ti–xAu (x = 5, 10, 15, 20, and 40 wt%) alloys to assess the effect of addition of element Au on the microstructure, mechanical properties, and corrosion behavior of commercially pure titanium (cp-Ti). The phase and microstructure were characterized using X-ray diffraction (XRD), optical microscopy, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The results indicated that the Ti–xAu alloys containing up to 15 wt% Au showed a hexagonal close-packed α-Ti structure, whereas the Ti–xAu alloys containing more than 20 wt% Au were mainly composed of the α-Ti phase and Ti3Au intermetallic phase. We also investigated the effect of alloying element Au on the mechanical properties (including Vickers hardness and modulus) and corrosion behavior of Ti–xAu binary alloys. The addition of gold to Ti improved its hardness. Electrochemical results showed that the Ti–xAu alloys exhibited improved corrosion resistance than cp-Ti.
In order to investigate the relationship between phase/microstructure and various properties of Ti–xAg alloys, a series of Ti–xAg alloys with Ag contents ranging from 5 to 20 wt% were prepared. The microstructures were characterized using X-ray diffractometry (XRD), optical microscopy (OM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). All of the Ti–xAg alloys showed a massive transformation from the β-Ti to αm phase, which has a different crystal structure from that of the matrix phase, but it has the same composition as the matrix α-Ti phase. As a result of solid-solution strengthening of α-Ti and massive transformation phase, the Ti–xAg showed better mechanical properties than the commercially pure titanium (cp-Ti). Electrochemical results showed that the Ti–xAg alloys exhibited improved corrosion resistance and oxidation resistance than cp-Ti.
1 September 2018 in Materials Science and Engineering: C