In this study, red-emitting Mn 4+ -activated CaAl 4 O 7 phosphors were successfully synthesized using a simple solid-state reaction method. The incorporation of Mn 4+ ions into the CaAl 4 O 7 lattice was confirmed by x-ray diffraction (XRD) analysis. The synthesized phosphors displayed a red emission band peaking at 656 nm, which can be tuned by adjusting the doping concentration and annealing temperature. The highest photoluminescence intensity was observed for the CaAl 4 O 7 :0.3%Mn 4+ sample annealed at 1500 °C. The optimized CaAl₄O₇:Mn 4+ phosphors exhibited a long lifetime of 0.827 ms, good color purity of 99.5% and high quantum efficiency of 49.7%. The plant growth LEDs were fabricated by combining the red-emitting optimized CaAl 4 O 7 :Mn 4+ phosphor with various LED chips emitting at 365, 395, 420, and 450 nm. The red phytochrome exhibits good alignment with the LED chips using UV and NUV excitation (around 365 nm and 395 nm), while chlorophyll A and B show strong correspondence with plant LED chips based on the violet (420 nm) and blue (450 nm) LED chips, respectively. Furthermore, high CRI warm white light-emitting diodes (W-WLEDs) were fabricated using the red-emitting CaAl 4 O 7 :Mn 4+ phosphor with a commercial yellow YAG:Ce 3+ and a 465 nm blue LED chip. Adding CaAl 4 O 7 :Mn 4+ significantly enhanced the CRI from 77 to 91, improved the R9 value from −15 to 84, and reduced the correlated color temperature from 5581 to 3998 K. The results indicate the significant potential of CaAl 4 O 7 :Mn 4+ phosphor for applications in both high CRI W-WLEDs and plant growth LEDs, effectively responding to red phytochrome and all chlorophyll absorption bands.
ZnS nanostructures possess exceptional features, making them highly promising as gain media and optical waveguides for nanolasers and optoelectronic devices. These features include low lasing thresholds and effortless fabrication. In this study, we present high-crystalline ZnS nanowires (NWs) and nanobelts (NBs) synthesized by using a thermal evaporation route. The remarkably low lasing thresholds of 45.3–45.5 W/cm2 are achieved at room temperature, marking a two-orders-of-magnitude improvement over reported values for ZnS nanostructures. Comprehensive analysis, incorporating techniques such as x-ray diffraction, Raman spectra, transmission electron microscopy, x-ray photoelectron spectroscopy, and photoluminescence, confirms the great quality of the synthesized nanostructures. The excitonic lasing emissions from ZnS NWs and NBs exhibit small full width at half maximum values of 5.9 and 0.53 nm, respectively. These emissions occur within cavities measuring ∼5.1 to 5.6 μm, with high-quality factors (112.6 for ZnS NWs and 598.6 for ZnS NBs), further highlighting the excellent performance of the materials. Moreover, the gain factors of 17.32–26.63 underscore the significant potential of ZnS NWs and NBs as prime candidates for ultraviolet photonic devices.
Eu 3+ -doped phosphors have attracted much interest due to the narrow-band red emission peaking at 610 ‒ 630 nm with high color purity; however, the weak and narrow absorption band in the NUV region limits their applications. Hence, the design of Eu 3+ -doped phosphors with a suitable host lattice is key for applications. In this work, red-emitting Eu 3+ -heavily doped Gd(BO 2 ) 3 -Y 3 BO 6 -GdBO 3 (GdYGd:Eu 3+ ) phosphor with a good quantum efficiency of 58.4% and high color purity of 99.5% is reported for the first time. The phosphor could be efficiently excited by NUV light at 394 nm and emits a strong red emission band in the range of 590-710 nm, peaking at 612 nm. The highest PL intensity is achieved at the annealing temperature of 1100 °C and the Eu 3+ doping concentration of 20 mol%. The optimized GdYGd:Eu 3+ phosphor possesses high activation energy of 0.319 eV and a long lifetime of 1.14 ms. A prototype of phosphor-coated NUV LED with the chromaticity coordinates (x = 0.5636; y = 0.2961) was successfully fabricated, demonstrating the great potential of GdYGd:Eu 3+ phosphor for NUV-pumped WLED applications.