1 January 2014 in AIP Conference Proceedings
Growth of Ba 0.5 Sr 0.5 TiO 3 (BST) 1 M thick films are conducted with variation of annealing hold time of 8 hours, 15 hours, 22 hours, and 29 hours at a constant temperature of 850 °C on p-type Si (100) substrate using sol-gel method then followed by spin coating process at 3000 rpm for 30 seconds. The BST thick film electrical conductivity is obtained to be 10−5 to 10−4 S/cm indicate that the BST thick film is classified as semiconductor material. The semiconductor energy band gap value of BST thick film based on annealing hold time of 8 hours, 15 hours, 22 hours, and 29 hours are 2.58 eV, 3.15 eV, 3.2 eV and 2.62 eV, respectively. The I-V photovoltaic characterization shows that the BST thick film is potentially solar cell device, and in accordance to annealing hold time of 8 hours, 15 hours, 22 hours and 29 hours have respective solar cell energy conversion efficiencies of 0.343%, 0.399%, 0.469% and 0.374%, respectively. Optical spectroscopy shows that BST thick film solar cells with annealing hold time of 8 hours, 15 hours, and 22 hours absorb effectively light energy at wavelength of ≥ 700 nm. BST film samples with annealing hold time of 29 hours absorb effectively light energy at wavelength of ≤ 700 nm. The BST thick film refraction index is between 1.1 to 1.8 at light wavelength between ±370 to 870 nm.
1 March 2015 in TELKOMNIKA (Telecommunication Computing Electronics and Control)
Design and Simulation of Quadrature Phase Detection in Electrical Capacitance Volume Tomography