Nanostructured nickel-iron-tungsten alloys were produced by electrodeposition from an ammoniacal citrate bath. The tungsten content of the alloy ranged from 0.8 wt.% to 11 wt.%, and the crystal grain size of the FCC phase of the solid solution of iron and tungsten in nickel was between 14 nm and 3.3 nm. The amorphous phase content of the alloy increases with decreasing crystal grain size. As the amorphous phase content increases, the magnetization, electrical conductivity and hardness of the alloy decrease. Annealing the alloy to crystallization temperature results in structural relaxation during which the alloy undergoes short-range ordering in conjunction with decreases in the density of chaotically distributed dislocations and internal microstrain level, which increases the exchange integral value, the electronic density of states at the Fermi level, the mean free path of electrons, the ordering and the mean size of cluster in the sliding plane and results in more uniform orientation of dipole moments of certain nanoparticles. These changes: a) increase the mobility of magnetic domain walls, facilitate the orientation of domains in the external magnetic field and cause an increase in magnetization; b) cause a decrease in electrical resistance, and c) impede the sliding of grain boundaries and increase the hardness of the alloy. Annealing the alloys at temperatures above 400?C results in amorphous phase crystallization and larger crystal grains of the FCC phase, along with a decrease in the density of chaotically distributed dislocations and a decrease in internal microstrain level. The formation of larger crystal grains reduces the hardness of the alloy, decreases its specific electrical resistance and impedes both the orientation of certain magnetic domains and the shift of walls of already oriented domains, thus inducing a decrease in magnetization. The heat released during the milling of Ni87.3Fe11.3W1.4 alloy with FCC-phase crystal grains 8.8 nm in average size causes amorphous phase crystallization, FCC crystal grain growth and an increase in magnetization. Alloys with relatively high tungsten content (11 wt. %) have an inhomogeneous composition, a high proportion of the amorphous phase and FCC crystal grains with an average size of 3.3 nm. This microstructure results in magnetic domains that have different and relatively low thermal stabilities and relatively low degrees of magnetization.
Cobalt and nickel powders of three different compositions: Ni0.8Co0.2, Ni0.55Co0.45 and Ni0.2Co0.8 were obtained by electrodeposition from an ammonium chloride-sulphate solution. It was shown that the microstructure and morphology of the powders depended on the deposition current density as well as on the bath composition. Amorphous powder of Ni0.8Co0.2 was obtained at the current density higher than 200 mA cm-2, but nanocrystalline powders having the same composition were obtained at current densities lower than 200 mAcm-2. The nanocrystalline powders with lower Ni contents (0.55 and 0.2) obtained at a current density ranging from 40 mA cm-2 to 450 mA cm-2 were solid solutions of two phases, FCC (?-Ni) and HCP (?-Co) ones. The increase of the HCP phase in the powder was a result of both the Co content increase in the powder and decrease of the deposition current density.
Nickel and molybdenum alloy powder was electrodeposited on a titanium cathode from a NiSO4?7H2O and (NH4)6 Mo7O24?4H2O ammonium solution. The desired chemical composition, structure, size and shape of particles in the powder samples were achieved by an appropriate choice of electrolysis parameters (current density, composition and temperature of the solution, cathode material and electrolysis duration). Metal coatings form in the current density range 15 mA cm-2
Chlorine is used worldwide for water disinfection purposes. However, due to its toxicity the EU has imposed a set of standards that must be applied when transporting and storing chlorine. In Serbia, numerous studies have been conducted attempting to develop the technology for the generation of active chlorine disinfectant but with a non-toxic aqueous solution of sodium chloride as the raw material. This study provides an overview of the titanium anodes activated by thermally obtained solid solution of ruthenium and titanium oxide development. It also presents new findings on the effect of the temperature of thermal treatment, the composition, the thickness of an active coating on its microstructural properties, and consequently on the catalytic activity, ion selectivity, and corrosion stability during active chlorine generation through the electrolysis of dilute sodium chloride solutions at room temperature. The study also evaluates the effect of the kinetic and operational parameters of the electrochemical process of active chlorine generation on both current and energy efficiencies. The results obtained were used to determine optimal values of technological parameters of the production process. This comprehensive research resulted in the construction of different types of remote-controlled and fully automated active chlorine generating plants.
1 January 2014 in Journal of the Serbian Chemical Society
A mathematical model has been set up for current efficiency in a chlorate cell acting as an ideal electrochemical tubular reactor with a linear increase in hypochlorite concentration from the entrance to the exit. Good agreement was found between the results on current efficiency experimentally obtained under simulated industrial chlorate production conditions and the theoretical values provided by the mathematical model.
Ni-Fe-W-Cu alloy powders were obtained by electrodeposition from an ammonium citrate bath at current densities ranging between 70 and 600 mA cm-2. As the deposition current density increased, the contents of Fe and W in the alloy increased, and those of Ni and Cu decreased. The total cathodic polarization curve was recorded, and partial polarization curves for Ni, Fe and W deposition and hydrogen evolution were determined. The current efficiency of alloy deposition was measured. The powders contained an amorphous matrix and FCC nanocrystals of the solid solution of Fe, W and Cu in Ni. At high current densities, small-sized nanocrystals exhibiting high internal microstrain values were formed. Powder particles were dendrite- and cauliflower-shaped. The dendrites had a large number of secondary branches and higher-order branches containing interconnected globules. The density of branches was higher in particles formed at high current densities. The powders formed at high current densities exhibited higher magnetization. Annealing at temperatures up to 460?C resulted in structural relaxation, accompanied by an increase in magnetization. At temperatures above 460?C, amorphous matrix crystallization and FCC crystal growth took place, accompanied by a decrease in magnetization.