A novel temperature gradient laboratory-scale corrosion test method was used to study PbCl2 migration, interactions with SiO2, NaCl, Na2SO4, KCl, K2SO4 or NaCl-KCl (50:50 wt-%), and corrosion of carbon steel in waste-fired boilers. Two different steel temperatures (200 °C and 400 °C) were tested. The temperature in the furnace above the deposits was 700-800 °C. Exposure times of 4 and 24h were used. The deposit cross-sections were analyzed using SEM/EDXA. The results show that PbCl2 vaporized and condensed in the adjacent deposits. PbCl2 did not interact with SiO2 but caused severe corrosion. Deposits containing Na2SO4, K2SO4 and/or KCl reacted with the PbCl2, forming various new compounds (Na3Pb2(SO4)3Cl, K3Pb2(SO4)3Cl and/or K2PbCl4). In addition, melt formation was observed with all alkali salt deposits. Visibly more Pb was found in deposits where reactions between PbCl2 and alkali salts were possible, i.e. Pb was observed to be bound to the reaction products. No measurable corrosion was observed with steel temperature at 200 °C, while steel temperature of 400 °C resulted in catastrophic corrosion. PbCl2 in contact with the steel surface lead to faster corrosion than K2PbCl4.
The aging of alkali bromide-containing ash deposits was studied by applying pre-mixed alkali bromide-alkali sulfate mixtures on a laboratory scale temperature gradient probe. The probe temperature was kept at 500 °C, while the furnace air temperature was measured to be 800 °C, simulating a heat exchanger ash deposit temperature profile. Deposits of ~5 mm thick were aged in the furnace for 2-8h and subsequently rapidly cooled to room temperature. The deposit cross sections were analyzed and characterized using SEM/EDX. The deposits were observed to form multilayered structures, where the furnace-facing region was dense and sintered, while the steel-facing region was porous. Within the porous region, a gas phase migration of alkali bromides towards the colder temperature was observed. The alkali bromide migration towards the colder steel temperature observed in the experiments was quantified and compared to modeling results. The modeling results were calculated by modifying an existing temperature gradient driven alkali chloride intradeposit migration model for alkali bromides. The model is in agreement with the experimental results, validating an enrichment mechanism for alkali bromides. Due to their relatively high saturation pressures, alkali bromide migration was observed to be significantly faster than the earlier reported migration of alkali chlorides. Enrichment of alkali bromides in colder temperatures in boiler deposits could lead to significant changes in the local composition of the deposit, possibly leading to enhanced corrosion rate of the tube material and/or densification of the deposit structure.