Arooj Rashid

Arooj Rashid

Auto-generated profile, based on publicly available information

Arooj Rashid

Department of Electrical and Computer Engineering (DECE), International Islamic University, Islamabad, 44000, Pakistan

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
9 April 2025 in Materials Advances
Verified
Journal Article
Open access
PDF file
FAFateha Aiman
Fateha Aiman
AKABRAIZ KHATTAK
ABRAIZ KHATTAK
ARArooj Rashid
Arooj Rashid
SBSafi Ullah Butt
Safi Ullah Butt
TATahira Arshad
Tahira Arshad
AAAbdulrehman Al-Arainy
Abdulrehman Al-Arainy
High temperature vulcanized (HTV) silicone rubber experiences deterioration in electrical performance when subjected to prolonged environmental stresses, limiting its effectiveness in insulation applications. This study investigates the electrical properties of HTV silicone rubber hybrid composites reinforced with nano-silica (2–10%) and micro-ATH (20%) under multi-stress aging for 9000 hours. The results show that hybrid composites exhibit improved electrical performance compared to neat silicone rubber. Notably, the SAT-6 composite displayed the highest DC resistivity (532.57 × 1013 Ω m) at 60 °C before aging, with only an 18.5% reduction after aging. SAT-2 demonstrated the smallest increase in the dielectric constant and tan δ, indicating better aging resistance. In contrast, SAT-10 showed the lowest resistivity and the highest increase in dielectric losses due to filler agglomeration and poor dispersion. Overall, leakage current increased after aging, but SAT-6 maintained the lowest value among all aged samples, while SAT-0 showed the highest. These results confirm that the optimal filler loading significantly enhances aging resistance, with up to 6.57% minimal loss in resistivity for SAT-6 at room temperature. These findings show the strong potential of HTV silicone rubber hybrid composites for industrial application in outdoor high-voltage insulation, where improved dielectric stability and long-term durability are critical, enabling reduced maintenance and enhanced reliability in power infrastructure.

26 January 2020 in Polymers and Polymer Composites
Verified
Journal Article
Closed access
PDF file
ARArooj Rashid
Arooj Rashid
JSJawad Saleem
Jawad Saleem
MAMuhammad Amin
Muhammad Amin
SASahibzada Muhammad Ali
Sahibzada Muhammad Ali
Multiple environmental stresses produce complex phenomena of aging in polymeric insulators. The main aim of this research is to investigate the improved aging characteristics of silica (SiO2)/alumina trihydrate (ATH) hybrid samples (HSs) in high-temperature vulcanized rubber. For this purpose, three HSs comprising 20% micro-ATH with 2% nano-SiO2 (S2), 4% nano-SiO2 (S4), 6% nano-SiO2 (S6) along with sample-virgin (SV) are subjected to long-term accelerated aging of 9000 h. A special aging chamber is fabricated for the aging process of samples. The aging characteristics of these samples are investigated by measuring leakage current (LC) and hydrophobicity classification (HC) after every weathering cycle. Similarly, Fourier transform infrared (FTIR) spectroscopy is performed to observe the important structural changes over the entire aging time. The dielectric strength of AC is also performed after every 1000 h of aging. Tracking and erosion resistance and mechanical properties are also investigated before and after aging. From the critical investigation, it is observed that HSs possess improved results in all the conducted tests. S2 has the lowest LC and HC values throughout the aging time. Similarly, S6 described the highest breakdown strength at the end of the accelerated aging. In the case of FTIR, it is analyzed that the important wave numbers remain intact for all the HSs in the accelerated aging environment. The loss percentage in the wave number for SV is higher, compared to the HSs. After performing the tracking and erosion resistance test, HSs have superior performance. For some of the mechanical properties, HSs showed improved values. Thus, from the experimental analysis, it is deducted that the sample S2 offers the highest resistance to the aging conditions, compared to the SV and other HSs.

1 July 2019
Verified
Conference Paper
Closed access
ARArooj Rashid
Arooj Rashid
JSJawad Saleem
Jawad Saleem
M. Asim AminM. Asim Amin
M. Asim Amin
With superior electrical properties, easy handling and low weight, polymeric materials are used for external insulating materials for outdoor and indoor applications. However, with the presence of environmental stresses such as contamination, and humidity in the environment, surface tracking and erosion may happen to polymeric insulating materials. Therefore, resistance of tracking of polymeric insulation materials is an important property to be investigated in recent years. Moreover, Polymer nano-composites/micro-composites have attracted wide interests in various industries. IEC 60587 standard (Inclined Plane Test (IPT)) gives a method for the evaluation of the tracking resistance in polymeric insulating materials. In this paper, the IPT method has been used to evaluate the performance of the polymeric insulators under AC voltages. Tests were conducted on polymer High Temperature Vulcanized Silicone Rubber (HTV-SiR) with fillers (nano+ micro silica) under AC stress. In this article, simultaneous addition of nano and micro sized filler is used to improve the erosion/tracking resistance of base material. Leakage Current, Initial Tracking Voltage (ITV), and Infrared thermographs are taken after every hours according to the IEC-10586 standard. After conducting test, overall Hybrid Samples have the improved resistance to tracking with the lowest leakage currents. However, among hybrid, sample EN1 (2% nano SiO2+20% micro SiO2) is the one with improved results. Leakage current, ITV and Infrared thermographs data support the above results.